Abstract

The invention relates to thermally tempered safety glass comprising an non-abrasive and porous SiO 2 layer which is stable during sintering and has a refractive index of between 1.25 and 1.40. The inventive safety glass can be obtained by coating standard soda-lime glass with an aqueous coating solution having a pH value of between 3 and 8 and containing between 0.5 and 5.0 wt. % of [SiO x (OH) y ] n particles (0<y<4 and 0<x<2) having a particle size of between 10 and 60 nm, and a surfactant mixture. The coated glass is then dried, thermally hardened at temperatures of at least 600° C. for several minutes, and thermally tempered by a flow of air.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a safety glass, comprising: coating a glass with an aqueous coating solution and a surfactant mixture, the aqueous coating solution having a pH of 3 to 8, containing 0.5 wt. % to 5.0 wt. % [SiO x (OH) y ] n particles, where 0<y<4 and 0<x<2 and n is an integer, the particles having a particle size of 10 nm to 60 nm so as to provide a coated glass; drying the coated glass; annealing the coated glass at temperatures of at least 600° C. for a period of 2 to 10 minutes; and tempering the coated glass in an air flow.

  2. Claim 2Depends on #1

    The method as recited in claim 1 , wherein the glass is a soda-lime glass.

  3. Claim 3Depends on #1

    The method as recited in claim 1 , wherein the drying includes one of resting the glass at room temperature and accelerated drying the glass using an air flow.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • A. Gombert et al., "Antireflective Transparent Covers for Solar Devices", Solar Energy vol. 4, pp. 357-360, 2000, Elsevier Science Ltd.
  • A. Gombert et al., "Glazing with Very High Solar Transmittance", Solar Energy vol. 62, No. 3, pp. 177-188, 1998, Elsevier Science Ltd.
  • A. Gombert et al., "Subwavelength-structured Antireflective Surfaces on Glass", Thin Solid Films (1999) 73-78, Elsevier Science S.A.
  • C.J. Brinker; G.W. Scherr, 'Sol-Gel Science', Academic Press 1990, p. 104, Fig. 5 and p. 583.
  • DIN 1249-12/prEN 12150, Nov. 2000, (discussed in specification).