Abstract
A spark plug includes a ceramic component, whose surface is at least in part coated with a glaze, with the glaze containing 0.6% to 4% by weight of fluoride and 6% to 11.2% by weight of zinc oxide.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 1.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for manufacturing a spark plug comprising: producing a glaze, wherein the production of the glaze includes blending a ceramic base with at least one of Kaolin and bentonite in such a manner that a thermal expansion coefficient of a fired glaze is <7 * 10 −6 1/K; and applying the glaze to ceramic components of the spark plug wherein the resulting spark plug has a head bending strength of at least 1800 Newtons.
- Claim 2Depends on #1
the method according to claim 1 , wherein the ceramic base is blended with up to at least one of (a) 5% by weight of bentonite and (b) 10% to 30% by weight kaolin.
- Claim 3Depends on #1
The spark plug according to claim 1 , further comprising melting the ceramic base at a temperature <900° C. after an addition of at least one of bentonite and kaolin.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 7,573,185 B2 | Small diameter/long reach spark plug with improved insulator design | 2009 | 2 |