Chemical vapor deposition chamber pre-deposition treatment for improved carbon doped oxide thickness uniformity and throughput
Abstract
A method for improving thickness uniformity and throughput of a carbon doped oxide deposition process is described. That method comprises removing pre-deposition steps in a deposition phase. Moreover, helium plasma is added to a pre-clean phase to eliminate the production of dummy wafers.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method comprising: applying a helium plasma treatment to a CVD chamber that includes a chamber wall and a spindle; cleaning the chamber walls with a first cleaning plasma after the helium plasma application; cleaning the spindle with a second cleaning plasma after the helium plasma application; and depositing a carbon doped oxide (CDO) film in the CVD chamber.
- Claim 2Depends on #1
The method of claim 1 , further comprising: post-cleaning the CVD chamber.
- Claim 3Depends on #1
The method of claim 1 , wherein the helium plasma treatment is applied for greater than one minute.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (11)
Non-Patent Literature (1)
- Andideh, et al., "Concentration Graded Carbon Doped Oxide," U.S. Appl. No. 09/943,874 filed Aug. 31, 2001. under Final Rejection.