Manufacturing method of semiconductor device
Abstract
When the occurrence of the bowing is controlled through the etching conditions, a change in etching conditions causes the bowing. Another problem is a requirement of the larger-sized apparatus for the substrate with a larger diameter in order to allow a whole substrate being subjected equally to the conditions under which no bowing occurs. In the present invention, a first etching is stopped at a depth where no bowing occurs to form an opening section. Next, a protective film for etching is formed on a region of the wall surface of the hole in the opening section where a bowing is liable to appear when an opening is formed further. After that, a second etching is carried out to form an opening further, and thereby a minute opening with an aspect ratio of 13 or higher is made, while suppressing the occurrence of the bowing well.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 10.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of manufacturing a semiconductor device to fabricate, by performing dry etching, an opening with an aspect ratio of not less than 13 in a first insulating film of an oxide of silicon which is formed on a basic substance so as to reach said basic substance; which comprises the steps of: performing a first etching to form an opening section which reaches a depth where no bowing occurs in said first insulating film; forming a sidewall made of a third insulating film, which has a lower etching rate than said first insulating film, to protect said wall surface wherein said sidewall covers
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗