US 7,122,403 B2#5835573 Most CitedExpiredUnited States (USPTO)Utility

Method of interconnecting die and substrate

16Forward Citations (#5835573 Global)
0.8/yrCitation Velocity (#9137756 Global)
2.60Citation PageRank (#9516151 Global)
43Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A low resistance package-to-die interconnect scheme for reduced die stresses includes a relatively low melting temperature and yield strength solder on the die and a relatively higher melting temperature and electrically conductive material such as copper on the substrate. A soldered joint connects the solder to the electrically conductive material to couple/connect the die and substrate to one another. The soldered joint is formed by heating the die and solder thereon to at least the melting temperature of the solder and thereafter contacting the molten solder with the conductive material on the substrate, which is at a substantially lower temperature for minimizing residual stress from soldering due to coefficient of thermal expansion mismatch between the substrate and die.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 43 · Forward citations: 16.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of interconnecting a die and a substrate to one another, the method comprising: heating a die having a relatively low melting temperature solder bump to a first temperature to form a reflowed solder bump; heating a substrate having a relatively higher melting temperature contact member to a second temperature that is lower than the first temperature; and joining the reflowed solder bump at the first temperature with the contact member at the second temperature to form a soldered joint.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the contact member is formed as a standoff extending above a surface of the substrate.

  3. Claim 3Depends on #2

    The method according to claim 2 , wherein the solder bump is wetted on a top surface of the standoff to form the soldered joint.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • ANONYMOUS, "Solder ball for semiconductor chip-has height increased so that stress caused by difference in thermal expansion between chip and substrate is minimised" Research Disclosure RD-291011, Derwent 1988-255069,(Jul. 10, 1988),2 pages.
  • Hong, B. Z., "Thermal Fatigue Analysis of CBGA Package with Lead-Free Solder-Fillets", Proceedings of the 1998 Intersociety Conference on Thermal Phenomena, (Aug., 1998),205-211.
  • Karim, Z. S., et al., "Lead-Free Bump Interconnections for Flip-Chip Applications", Proceedings of the 2000 IEEE/CPMT International Electronics Manufacturing Technology Symposium, (Jan., 2000),274-278.
  • Wang, T. , et al., "Studies on A Novel Flip-Chip Interconnect Structure-Pillar Bump", Proceedings of the 2001 Electronic Components and Technology Conference, (Apr., 2001),5 p.
  • Xia, G. , et al., "The Effect of Cu Stud Structure and Eutectic Solder Electroplating on Intermetallic Growth and Reliability of Flip-Chip Solder Bump", Proceedings of the 2000 Electronic Components and Technology Conference, (Sep., 2000),54-59.