Patents
US 7,121,402 B2#4211784 Most CitedExpiredUnited States (USPTO)Utility

Container hermetically sealed with crushable material and reactive multilayer material

20Forward Citations (#4211784 Global)
1.0/yrCitation Velocity (#6263382 Global)
3.54Citation PageRank (#5809246 Global)
29Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the invention include a method for sealing a container. The method includes, providing at least two components of the container, positioning a crushable material between the at least two components, positioning a reactive multilayer material between the at least two components, deforming the crushable material so as to form a seal between the at least two components, chemically transforming the reactive multilayer material so as to join the at least two components.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 20.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A sealed product, comprising: at least two components defining a container including a sealed interior cavity; a crushable material disposed between the at least two components, the crushable material being in a deformed state and forming a seal between the at least two components; and a fusible material and a remnant of a chemical transformation of a reactive multilayer material disposed between the at least two components and joining said at least two components.

  2. Claim 2Depends on #1

    The sealed product of claim 1 , wherein the reactive multilayer material includes a reactive multilayer foil.

  3. Claim 3Depends on #1

    The sealed product of claim 1 , wherein the crushable material and the remnant of the chemical transformation cooperate to form a hermetic seal between the at least two components.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Technique for Obtaining an Environmentally Secure Adhesive Seal"; IBM Technical Disclosure Bulletin; Dec. 1, 1986; pp. 3085-3087; vol. 29, No. 7; XP002025799; ISSN: 0018-8689; IBM Corp.; New York, US.
  • A.J. Gavens, D. Van Heerden, A.B. Mann, M.E. Reiss, and T.P. Weihs; "Effect of Intermixing on Self-Propagating Exothermic Reactions in Al/Ni Nanolaminate Foils"; Journal of Applied Physics; Feb. 1, 2000; pp. 1255-1263; vol. 87, No. 3.
  • A.J. Swiston Jr., T.C. Hufnagel, and T.P. Weihs; "Joining Bulk Metallic Glass Using Reactive Multilayer Foils"; Scripta Materialia; 2003; pp. 1575-1580; vol. 48.
  • D. Josell, A. Cezairliyan, D. Van Heerden, and B.T. Murray; "Thermal Diffusion Through Multilayer Coatings: Theory and Experiment"; NanoStructured Materials; 1997; pp. 727-736; vol. 9 Nos. 1-8.
  • D. Van Heerden, A.J. Gavens, S. Jayaraman, and T.P. Weihs; "Metastable Phase Formation and Microstructural Evolution During Self-Propagating Reactions in Al/Ni and Al/Monel Multilayers"; Material Research Society Symposium Proceedings; Fall 1997; pp. 533-538; vol. 481.