US 7,115,685 B2#33490204 Most CitedExpiredUnited States (USPTO)Utility

Fluoropolymer-carbon dioxide compositions and methods of processing fluoropolymers

3Forward Citations (#33490204 Global)
0.1/yrCitation Velocity (#38814905 Global)
1.03Citation PageRank (#39867056 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Fluoropolymer materials containing tetrafluoroethylene monomers, such as PTFE, are significantly swollen by supercritical carbon dioxide at high temperatures and pressures. The swollen fluoropolymer is processable by molding, extrusion, and other techniques. In addition, the fluoropolymer may be sintered at significantly lower temperatures compared to a nonswollen fluoropolymer material. The melting temperature of fluorinated polymers containing tetrafluoroethylene and triflouroethylene monomers which are swollen with supercritical carbon dioxide is significantly reduced, thereby permitting manufacturing operations such as extruding and molding to be performed at lower temperatures and with reduced risk of decomposition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for processing polychlorotrifluoroethylene (PCTFE), comprising the steps of: exposing PCTFE to supercritical carbon dioxide at 8,000 psi; lowering the melting point of said PCTFE to 150° C.; and performing a manufacturing operation on said PCTFE above said melting temperature.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (2)

Non-Patent Literature (1)

  • International Standard ISO12086-1, First Edition, 1995, p. 1.