Patents
US 7,109,092 B2#2170573 Most CitedExpiredUnited States (USPTO)Utility

Method of room temperature covalent bonding

31Forward Citations (#2170573 Global)
1.6/yrCitation Velocity (#3310829 Global)
3.98Citation PageRank (#4797272 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of bonding includes using a bonding layer having a fluorinated oxide. Fluorine may be introduced into the bonding layer by exposure to a fluorine-containing solution, vapor or gas or by implantation. The bonding layer may also be formed using a method where fluorine is introduced into the layer during its formation. The surface of the bonding layer is terminated with a desired species, preferably an NH 2 species. This may be accomplished by exposing the bonding layer to an NH 4 OH solution. High bonding strength is obtained at room temperature. The method may also include bonding two bonding layers together and creating a fluorine distribution having a peak in the vicinity of the interface between the bonding layers. One of the bonding layers may include two oxide layers formed on each other. The fluorine concentration may also have a second peak at the interface between the two oxide layers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 31.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A bonding method, comprising: forming first and second bonding layers on respective first and second elements, at least one of said bonding layers comprising a fluorinated oxide layer; heating said fluorinated oxide layer; after said heating, bringing into contact said first and second bonding layers in ambient at room temperature; and forming a bond between said first and second layers at room temperature.

  2. Claim 2Depends on #1

    A method as recited in claim 1 , comprising: forming a bond of at least 600 mJ/m 2 at room temperature.

  3. Claim 3Depends on #1

    A method as recited in claim 1 , comprising: forming a bond of at least 1000 mJ/m 2 at room temperature.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • A. Kazor et al., Appl. Phys. Lett. 65 (1994) p. 1572.
  • H. Nielsen et al., J. Electrochem. Soc. 130 (1983) p. 708.
  • J. Song et al., Appl. Phys. Lett. 69 (1996) p. 1876.
  • J.C.C. Tsai et al., VLSI Technology, McGraw-Hill, Auckland (1983), p. 147.
  • K.M. Chang et al., Appl. Phys. Lett. 69 (1996) p. 1238.