A spun polyester fiber, a drawn polyester yarn, and methods for making them. Polyethylene terephthalate yarn is prepared by extruding a molten melt-spinnable polyethylene terephthalate having an intrinsic viscosity of at least about 0.8 through a shaped extrusion orifice having a plurality of openings to form a molten spun yarn; solidifying gradually said molten spun yarn by passing said molten spun yarn through a solidification zone which comprises (i) a retarded cooling zone and (ii) a cooling zone adjacent said retarded cooling zone where, in said cooling zone, said yarn is rapidly cooled and solidified in a gaseous atmosphere; withdrawing at sufficient speed said solidified yarn from said solidification zone to form a crystalline partially oriented yarn; and hot drawing said crystalline partially oriented yarn at a total draw ratio between about 1.5/1 and about 2.5/1 to produce a drawn yarn having an effective crosslink density (N) between about 10×10 21 and about 20×10 21 crosslinks per cubic centimeter. The yarns and fibers so prepared may be used to make treated tire cord having high tenacity in combination with improved dimensional stability.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the production of a drawn polyethylene terephthalate yarn which translates to a high tenacity dimensionally stable tire cord, the process comprising: (a) extruding a molten melt-spinnable polyethylene terephthalate having an intrinsic viscosity of at least about 0.8 through a shaped extrusion orifice having a plurality of openings to form a molten spun yarn; (b) solidifying gradually said molten spun yarn by passing said molten spun yarn through a solidification zone which comprises (i) a retarded cooling zone and (ii) a cooling zone adjacent said retarded cooling zone, wherein s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
US 3,690,362 AHigh strength polyethylene terephthalate yarn and cord produced therefrom197216
JP S5196521 ANetsukasoseijugotaino kosokuboshiho—6
US 4,101,525 APolyester yarn of high strength possessing an unusually stable internal structure197896
US 4,195,052 AProduction of improved polyester filaments of high strength possessing an unusually stable internal structure198056
JP S561986 APattern generator—1
US 4,251,481 AContinuous spin-draw polyester process198146
EP 0,080,906 A2Polyester fibres and their production—27
EP 0,089,912 A2Process for the production of high-strength polyester yarn—17
US 4,414,169 AProduction of polyester filaments of high strength possessing an unusually stable internal structure employing improved processing conditions198362
JP S58203112 AProduction of polyester fiber—4
JP S59116414 APolyester yarn for reinforcing rubber—8
US 4,491,657 APolyester multifilament yarn and process for producing thereof1985105
EP 0,169,415 A2Polyester fiber—23
US 4,690,866 APolyester fiber198737
US 4,827,999 APolyester fiber having excellent thermal dimensional _ stability, chemical stability and high _ tenacity and process for the production thereof198945
US 4,867,936 AProcess for producing high strength polyester yarn for improved fatigue resistance198931
US 4,975,326 AHigh strength polyester yarn for improved fatigue resistance199032
US 5,132,067 AProcess for production of dimensionally stable polyester yarn for highly dimensionally stable treated cords199226
US 5,234,764 ADimensionally stable polyester yarn for high tenacity treaty cords199338
US 5,350,632 AImpregnated, dimension-stable polyester cord199414
US 5,630,976 AProcess of making dimensionally stable polyester yarn for high tenacity treated cords199739
US 6,403,006 B1Process of making dimensionally stable polyester yarn for high tenacity treated cords200211

Non-Patent Literature (5)

  • "A Study of Structural Development in the High SpeedSpinning of Poly(ethylene Terephthalate)" by H.H. George, A. Holt, and A. Buckley; Polymer Engineering & Science Mid-Feb., 1983, vol. 23, No. 2, pp. 95-99.
  • "High Speed Spinning of Polyethylene Terephthalate (PETP) by Pneumatic Take-up. Physical and Mechanical Properties of Filaments" by G. Perez and C. Lecluse, International Chemifasertagung in Dornbirn Conference, Jun. 20-22, 1979, conference pp. 1-37.
  • A. Roos, "Melt Spinning of PET Industrial Fibers", Fiber Formation Symposium, ACS Meeting, Toronto, Canada (Jun. 5-10, 1988).
  • After Appeal, First Korean Brief filed Apr. 21, 2000 by AlliedSignal Inc.
  • Decision of European Technical Board of Appeal Maintaining European Patent 423,123 Dated Sep. 23, 1999.