Anti-reflection film and process for the preparation of the same
Abstract
An anti-reflection film comprises a transparent support and a low refractive index coating layer. The low refractive index coating layer has a refractive index lower than a refractive index of the support. The low refractive index coating layer has an essentially uniform thickness, while the layer has a surface roughness in terms of an arithmetic mean (Ra) in the range of 0.05 to 2 μm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 22.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for the preparation of an anti-reflection film comprising the steps of: forming a hard coating layer on a transparent support; coating a coating solution on the hard coating layer to form a low refractive index layer having an essentially uniform thickness in the range of 50 to 400 nm and a surface roughness in terms of an arithmetic mean in the range of 0.05 to 2 m, wherein the low refractive index layer comprises inorganic particles, a cross-linked binder polymer and a silane coupling agent, said inorganic particles being surface treated with the silane coupling agent, and said sil
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗