Patents
US 7,105,141 B2#36941859 Most CitedExpiredUnited States (USPTO)Utility

Process and apparatus for the manufacture of carbon microballoons

2Forward Citations (#36941859 Global)
0.1/yrCitation Velocity (#45465396 Global)
1.14Citation PageRank (#34921984 Global)
17Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

This invention provides a stepped heating cycle for the pre-treatment of phenolic microballoons prior to carbonization thereof, wherein the heating cycle comprises the steps of sequentially: gradually elevating the temperature of the microballoons to a temperature in the range 100° C.–170° C.; holding the microballoons at the elevated temperature for 1–24 hours; and gradually cooling the microballoons. This invention also provides a heat-dissipation reactor ( 11, 21, 31 ) which comprises a walled reaction chamber having a bottom and no top, the reaction chamber being fitted with high thermal conductivity inserts. When used in accordance with this invention ( 61 ), the volume within the walls of the reaction chamber is charged with phenolic resin microballoons. In a preferred embodiment, the reaction chamber ( 11, 21 ) is subdivided into a plurality of subchambers by a vertical grid of aluminum plates ( 19, 29 ). In this embodiment, about half or more of the wall area of each subchamber comprises aluminum and a top edge ( 17 ) of the aluminum wall material communicates with atmosphere above the reaction chamber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 2.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A batch process for manufacturing carbon microballoons, comprising the steps of: providing cured phenolic resin microballoons; gradually elevating the temperature of the microballoons to a temperature in the range 100° C.–170° C. in a heat-dissipation reactor; holding the microballoons at the elevated temperature for 1–24 hours; gradually cooling the microballoons; and subsequently removing the phenolic microballoons from the heat-dissipation reactor, placing them into a graphite reactor, and heating them in an inert atmosphere to convert the phenolic microballoons into carbon microballoons.

  2. Claim 2Independent Claim

    A stepped heating cycle for the pre-treatment of phenolic microballoons prior to carbonization thereof, wherein the heating cycle comprises the steps of sequentially: raising the temperature of the microballoons to approximately

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗