US 7,101,594 B2#72637557 Most CitedExpiredUnited States (USPTO)Utility

Methods of forming capacitor constructions

0Forward Citations (#72637557 Global)
0.0/yrCitation Velocity (#72637557 Global)
0.56Citation PageRank (#72637557 Global)
18Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention includes a method of treating a predominantly inorganic dielectric material on a semiconductor wafer. A laser is utilized to generate activated oxygen species. Such activated oxygen species react with a component of the dielectric material to increase an oxygen content of the dielectric material. The invention also includes a method of forming a capacitor construction. A first capacitor electrode is formed to be supported by a semiconductor substrate. A dielectric material is formed over the first capacitor electrode. A precursor is provided at a location proximate the dielectric material, and a laser beam is focused at such location. The laser beam generates an activated oxygen species from the precursor. The activated oxygen species contacts the dielectric material. Subsequently, a second capacitor electrode is formed over the dielectric material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a capacitor construction comprising: forming a capacitor electrode supported by a semiconductor substrate; depositing a metal oxide dielectric material over the capacitor electrode; providing a precursor at a location proximate the metal oxide dielectric material; laser generating at least one activated species from the precursor; and after the laser generating, contacting the at least one activated species with the dielectric material.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the metal oxide dielectric material comprises one or more of tantalum pentoxide, aluminum pentoxide, hafnium oxide, titanium oxide, strontium titanate, barium strontium titanate and silicon oxynitride.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the at least one activated species comprises an activated oxygen species.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • Cranciun et al., "Low Temperature Growth of Barium Strontium Titanate Films by Ultraviolet-Assisted Pulsed Laser Deposition", Mat. Res. Symp. vol. 617, pp. J3.21.1-J3.21.6, 2000. Year is sufficiently early such that the month is not an issue.