Silicon strain engineering accomplished via use of specific shallow trench isolation fill materials
Abstract
A method of forming a strained silicon layer created via a material mis-match with adjacent trench isolation (TI), regions filled with a dielectric layer comprised with either a higher, or lower thermal expansion coefficient than that of silicon, has been developed. Filling of trenches with a dielectric layer comprised with a higher thermal expansion coefficient than that of silicon results in a tensile strain in planar direction and compressive strain in vertical direction, in an adjacent silicon region. Enhanced electron mobility in channel regions of an N channel MOSFET device, and enhanced hole mobility and transit time in an N type base region of a vertical PNP bipolar device, is realized when these elements are formed in the silicon layer under tensile strain. Filling of trenches with a dielectric layer comprised with a lower thermal expansion coefficient than the thermal expansion coefficient of silicon results in a compressive strain in planar directions and tensile strain in vertical directions, in an adjacent silicon region. Enhanced hole mobility in channel regions of an P channel MOSFET device, and enhanced electron mobility and transit time in a P type base region of a
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 21.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of forming trench isolation (TI) regions in a semiconductor substrate to create strained regions, comprising: defining first trenches and second trenches in the semiconductor substrate to surround active regions; filling the first trenches with a first dielectric layer and the second trenches with a second dielectric layer to form said TI regions, wherein a first active region among the active regions abuts one of the first trenches and one of the second trenches, wherein the active regions have a thermal expansion coefficient less than the thermal expansion coefficient of the first d
- Claim 2Depends on #1
The method as claimed in claim 1 , wherein the step of filling the first trenches with the first dielectric layer a
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗