Abstract

A defect free semipermeable composite membrane having excellent integrity and high water permeability is provided. Said composite membrane comprises an inside support layer to provide sufficient mechanical strength; an outside barrier layer to provide selective separation; and a middle layer to provide both physical adhesion and chemical binding between said support and said barrier layer to bond them together. Three different methods for making said defect free composite membrane are discovered. These methods have been successfully utilized to produce high quality coatings and defect free composite membranes, which are independent of chemical composition and physical structure of said support. In the present invention, ultrasonic sonication is discovered to be effective to speed up the phase inversion process of a membrane casting solution, thus allows produce a composite membrane at a speed much higher than those disclosed in the prior art. Said defect free composite membranes have broad applications, ranging from filtration of fruit juice, wine and milk to biotech down stream processing and purification of drinking water, municipal and industrial wastewater.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing a defect free composite membrane comprising: (i) preparing a solution A comprising a chemical, which are selected from the group consisting of epoxy, polyurethane, silicone, adhesives, monomers, polymers, and combinations thereof; (ii) preparing a solution B comprising 8–60% of a hydrophobic polymer, 1–20% of a hydrophilic polymer, 1–20% of inorganic additive, 1–10% of monomers, 1–10% of organic additives, and solvents; (iii) providing a support; (iv) coating said support at a speed from 5 to 3,000 ft/min with solution A and solution B simultaneously using a spinneret; w

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (16)