Patents
US 7,078,096 B2#20314809 Most CitedExpiredUnited States (USPTO)Utility

Method for producing polyester extra fine multi-filament yarn and polyester extra fine false twist textured yarn, polyester extra fine multi-filament yarn, and polyester extra-fine false twist textured yarn

5Forward Citations (#20314809 Global)
0.2/yrCitation Velocity (#28334734 Global)
1.61Citation PageRank (#20403452 Global)
12Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

There are provided a process for producing a polyester fine multifilament yarn having a single filament fineness of 0.9 dtex or below, a total number of single filaments of 100 to 400 and a birefringence of 0.03 to 0.06 comprising passing polymer streams of a polyester polymer melt extruded from a spinneret surface through an atmosphere wherein a distance of 0 to 40 mm from the spinneret surface is regulated to a temperature within the range of 100 to 300° C., further cooling the polymer streams and then converging the cooled filaments into a filament bundle at a position of 350 to 500 mm from the spinneret surface; a process for producing a polyester fine false twist textured yarn comprising subjecting a polyester fine multifilament yarn having a single filament fineness of 0.9 dtex or below, a total number of single filaments of 100 to 400 and a bifringence of 0.03 to 0.06 to false twist texturing, the process comprising subjecting the multifilament yarn to air interlacing so as to provide a degree of interlacing of 50 to 90 interlaced spots/m measured for the false twist textured yarn, regulating the residence time in a draw-false twisting heater of 0.052 to 0.300 second and the

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a polyester fine false twist textured yarn composed of a polyester and having a single filament fineness of 0.6 dtex or below and a total number of single filaments of 100 to 400 and satisfying the following (i) to (l): (i) a total crime ratio TC of 2 to 5%, (j) a shrinkage percentage in boiling water FS of 2.5 to 4.5%, (k) a breaking strength of 3.0 cN/dtex or above and (l) a breaking elongation of 15 to 45%, comprising subjecting a polyester fine multifilament yarn having a single filament fineness of 0.9 dtex or below, a total number of single filaments of 100 and 40

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗