Methods of fabricating self-aligned source of flash memory device
Abstract
Example methods of fabricating semiconductor devices are disclosed. One example method may include depositing an oxide layer, a first conducting layer for a floating gate, a dielectric layer, and a second conducting layer for a control gate in sequence on a semiconductor substrate including a device isolation layer; forming gates by removing some parts of the oxide layer, the first conducting layer, the dielectric layer, and the second conducting layer; forming a mask pattern for a self-aligned source over the substrate including the gates; removing the device isolation layer exposed between the gates; performing an ion implantation process; and eliminating damage generated during the ion implantation process or the removal of the device isolation layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of fabricating a semiconductor device comprising: depositing an oxide layer, a first conducting layer for a floating gate, a dielectric layer, and a second conducting layer for a control gate in sequence on a semiconductor substrate including a device isolation layer; forming gates by removing some part of the oxide layer, the first conducting layer, the dielectric layer, and the second conducting layer; forming a mask pattern for a self-aligned source over the substrate including the gates; removing the device isolation layer exposed between the gates; performing an ion implantation
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| CN 108,987,401 A | A kind of technology integrating method improving flash cell erasing state uniformity | — | 1 |