US 7,074,286 B2#16024375 Most CitedExpiredUnited States (USPTO)Utility

Wrought Cr—W—V bainitic/ferritic steel compositions

7Forward Citations (#16024375 Global)
0.3/yrCitation Velocity (#22467152 Global)
1.40Citation PageRank (#25486175 Global)
10Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A high-strength, high-toughness steel alloy includes, generally, about 2.5% to about 4% chromium, about 1.5% to about 3.5% tungsten, about 0.1% to about 0.5% vanadium, and about 0.05% to 0.25% carbon with the balance iron, wherein the percentages are by total weight of the composition, wherein the alloy is heated to an austenitizing temperature and then cooled to produce an austenite transformation product.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A high-strength, high-toughness wrough steel composition comprising: about 2.5% to about 4% chromium, about 1.5% to less t 2.15% tungsten, about 0.1% to about 0.5% vanadium, about 0.2% to about 1.5% manganese, and from 0.50% molybdenum to the lesser of 1.0% molybdenum and ½ (3.5%—said weight % of said tungsten), and about 0.05% to 0.25% carbon with the balance being iron, wherein the percentages are by total weight of the composition, and wherein a yield strength (YS) at room temperature of said steel is from 805 to 1024 MPa.

  2. Claim 2Depends on #1

    A wrought steel composition in accordance with claim 1 wherein a microstructure of said steel comprises carbide-free acicular bainite.

  3. Claim 3Depends on #1

    A wrought steel composition in accordance with claim 1 further comprising 0.07% to about 0.25% tantalum.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗