Method of identifying defect distribution in silicon single crystal ingot

6Forward Citations (#17256557 Global)
0.3/yrCitation Velocity (#25529177 Global)
1.79Citation PageRank (#17361606 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A surface of a reference sample is contaminated with a transition metal, and a heat treatment is performed to diffuse the transition metal in the sample. A concentration of recombination centers formed by the transition metal is measured in the entire heat-treated reference sample, and a region [V], a region [Pv], a region [Pi], and a region [I] in the reference sample are defined based on the values measured. Meanwhile, recombination lifetimes associated with the transition metal are measured in the entire heat-treated reference sample. Based on both of the measurement results, a correlation line of the concentration of recombination centers and the recombination lifetimes is produced. A surface of the measurement sample is contaminated with the transition metal, and a heat treatment is performed to diffuse the transition metal in the sample. Recombination lifetimes associated with the transition metal are measured in the entire heat-treated measurement sample, and the values measured are checked against the correlation line to infer the region [Pv] and the region [Pi] as well as the boundary thereof in the measurement sample.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 6.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of identifying a point defect distribution in a silicon single crystal ingot, comprising the steps of: (a) slicing a first silicon single crystal ingot in an axial direction thereof, the ingot pulled from a first silicon melt at a varying pull rate, to prepare a reference sample including a region [V], a region [Pv], a region [Pi], and a region [I]; (b) coating a surface of the reference sample with a transition metal solution in which a transition metal is dissolved at a concentration of 1 to 1000 ppm to metal-contaminate the reference sample; (c) heat-treating the metal-contaminated