US 7,071,072 B2#25980846 Most CitedExpiredUnited States (USPTO)Utility

Forming shallow trench isolation without the use of CMP

4Forward Citations (#25980846 Global)
0.2/yrCitation Velocity (#32869573 Global)
1.25Citation PageRank (#30236758 Global)
18Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Shallow trench isolation structures are formed without CMP by depositing a thick pad nitride and depositing oxide trench fill material such that: a) the material in the trenches is above the silicon surface by a process margin that allows for removal of trench fill in subsequent front end steps so that the final trench fill level is substantially coplanar with the silicon; and b) the oxide on the interior walls is easily removed, so that the pad nitride is removed in a wet etch.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a set of insulator plugs in an isolation trench in a semiconductor substrate having a device layer, without the use of CMP, comprising the steps of: depositing a pad insulator layer having a pad thickness over said device layer surface; etching a set of isolation apertures through said pad insulator and said device layer to an isolation depth; depositing in a single deposition step an isolation insulator layer in said isolation apertures to a depth sufficient to fill said isolation apertures above said device layer by a first margin that is less than the thickness of said p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Stanley Wolf, Silicon Processing For The VLSI Era, 1986, Lattice Press, vol. II, pp. 66-67.