Patents
US 7,071,069 B2#4949138 Most CitedExpiredUnited States (USPTO)Utility

Shallow amorphizing implant for gettering of deep secondary end of range defects

18Forward Citations (#4949138 Global)
0.9/yrCitation Velocity (#7931140 Global)
2.87Citation PageRank (#8130163 Global)
14Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A pocket implant process to reduce defects. We provide a gate structure, on a semiconductor substrate doped with a first conductivity type dopant. We perform a pocket amorphizing implantation procedure to form a pocket implant region adjacent to the gate structure, and an amorphous pocket region. Next, we perform a shallow amorphizing implant to form an amorphous shallow implant region. The amorphous shallow implant region being formed at a second depth above the amorphous pocket region. The substrate above the amorphous shallow implant region preferably remains crystalline. We perform a S/D implant procedure to form Deep S/D regions. We perform an anneal procedure preferably comprised of a first soak step and a second spike step to recrystalilze the amorphous shallow implant region and the amorphous pocket region, The defects created by the pocket implant are reduced by the shallow amorphous implant.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 18.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming an amorphous shallow implant region that getters defects from a pocket implantation; comprising: a) providing a gate structure, on a substrate comprised with a first conductivity type dopant; said substrate comprised of an upper crystalline section; b) performing a pocket amorphizing implantation procedure to implant ions of a first conductivity type to form a pocket implant region adjacent to said gate structure, and an amorphous pocket region; (1) said amorphous pocket region is formed at a first depth below the substrate surface; c) performing a shallow amorphizing imp

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)

PatentTitleYearCitations
US 2006134874 A1Manufacture method of MOS semiconductor device having extension and pocket—7
US 2009286373 A1Method for fabricating semiconductor devices with shallow diffusion regions—13
US 8,741,710 B2Methods of fabricating semiconductor devices using a plasma process with non-silane gas including deuterium20140
US 8,324,011 B2Implementation of temperature-dependent phase switch layer for improved temperature uniformity during annealing20124
US 2009087971 A1Method for fabricating semiconductor devices with reduced junction diffusion—16
US 9,984,917 B2Semiconductor device with an interconnect and a method for manufacturing thereof20180
US 7,855,118 B2Drive current increase in transistors by asymmetric amorphization implantation20101
US 7,994,016 B2Method for obtaining quality ultra-shallow doped regions and device having same20111
US 8,101,487 B2Method for fabricating semiconductor devices with shallow diffusion regions20121
US 2009298249 A1Drive current increase in transistors by asymmetric amorphization implantation—13
US 8,354,321 B2Method for fabricating semiconductor devices with reduced junction diffusion20130
US 7,358,167 B2Implantation process in semiconductor fabrication20082
US 2009068825 A1Implementation of temperature-dependent phase switch layer for improved temperature uniformity during annealing—3
US 2015340277 A1Method for manufacturing a semiconductor device and semiconductor device—6
US 2009104741 A1Methods of fabricating semiconductor devices using a plasma process with non-silane gas including deuterium—18

Non-Patent Literature (4)

  • Lisebarger, et al., "Study of end of range loop interactions with B[sup+ ] implant damage using a boron doped diffusion layer", J. Appl. Phys. 78 (4), Aug. 15, 1995, pp. 2298-2302.
  • Lu et al., "Reduction of secondary defect formation in MeV B+ ion-implanted Si(100)", Appl. pHys. Lett, 655 (18), Oct 30, 1989, pp. 1838-1840.
  • Noda, "Evolution of end-of-range damage and transient enhanced diffusion of indium in Silicon", Journal-of applied physics, vol. 91, #2 Jan. 15, 2002, pp. 639-645.
  • Yeh et al., Optimum halo structure for sub-0.1. m cMOSFETs, IEEE trans on electronic devices, vol. 48, # 10, Oct. 2001, pp. 2357-2362.