Patents
US 7,071,066 B2#5449844 Most CitedExpiredUnited States (USPTO)Utility

Method and structure for forming high-k gates

17Forward Citations (#5449844 Global)
0.8/yrCitation Velocity (#8599849 Global)
2.19Citation PageRank (#12604241 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for forming an improved gate stack structure having improved electrical properties in a gate structure forming process A method for forming a high dielectric constant gate structure including providing a silicon substrate comprising exposed surface portions; forming an interfacial layer over the exposed surface portions having a thickness of less than about 10 Angstroms; forming a high dielectric constant metal oxide layer over the interfacial layer having a dielectric constant of greater than about 10; forming a barrier layer over the high dielectric constant metal oxide layer; forming an electrode layer over the barrier layer; and, etching according to an etching pattern through a thickness of the electrode layer, barrier layer, high dielectric constant material layer, and the interfacial layer to form a high dielectric constant gate structure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 17.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming a gate stack having improved electrical properties in a gate structure forming process comprising the steps of: providing a semiconductor substrate; forming a metal oxide layer over an exposed portion of the semiconductor substrate; and forming a silicon-containing electrode layer over the metal oxide layer by depositing a silicon layer and introducing a nitrogen containing ambient simultaneously.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the metal oxide layer comprises a dielectric constant of greater than about 20.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the metal oxide is formed having a thickness of about 20 Angstroms to about 100 Angstroms.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗