Patents
US 7,067,022 B2#16144407 Most CitedExpiredUnited States (USPTO)Utility

Method for protecting a surface

7Forward Citations (#16144407 Global)
0.3/yrCitation Velocity (#22481022 Global)
1.28Citation PageRank (#29274495 Global)
23Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention includes a method of producing a hard metallic material by forming a mixture containing at least 55% iron and at least one of B, C, Si and P. The mixture is formed into an alloy and cooled to form a metallic material having a hardness of greater than about 9.2 GPa. The invention includes a method of forming a wire by combining a metal strip and a powder. The strip and the powder are rolled to form a wire containing at least 55% iron and from 2–7 additional elements including at lease one of C, Si and B. The invention also includes a method of forming a hardened surface on a substrate by processing a solid mass to form a power, applying the powder to a surface to form a layer containing metallic glass, and converting the glass to a crystalline material having a nanocrystalline grain size.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a hardened surface on a substrate, comprising: providing a solid mass comprising a first hardness; processing the solid mass to form a powder; combining the powder with a metal strip to form a wire, the wire having a final composition comprising at least 55% iron by weight and at least one element selected from the group consisting of Si, C, P and B; applying the final composition to a surface of a substrate to initially form a layer having a second hardness, at least some of the layer comprising metallic glass, the applying comprising at least one of twin-roll wire arc dep

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (23)

PatentTitleYearCitations
US 4,365,994 AComplex boride particle containing alloys198287
US 4,439,236 AComplex boride particle containing alloys198459
US 4,725,512 AMaterials transformable from the nonamorphous to the amorphous state under frictional loadings198873
JP S63219553 ABending method for amorphous fine metallic wire—2
US 4,820,141 AMethod for the manufacture of formed products from powders, foils, or fine wires198932
US 4,822,415 AThermal spray iron alloy powder containing molybdenum, copper and boron1989125
JP H02170950 AAmorphous magnetic alloy material—3
JP H055164 AIron base soft magnetic alloy—6
JP H05271885 ASoft magnetic alloy thin film and its manufacture—5
JP H0641675 AManufacture of amorphous bulk magnetic material—1
US 5,294,462 AElectric arc spray coating with cored wire199487
JP H08323480 AMethod for connecting fine wire of amorphous alloy to conductor—2
JP H093608 AIron-base soft-magnetic alloy and iron-base soft-magnetic alloy foil—2
US 5,643,531 AFerrous alloy composition and manufacture and coating methods of mechanical products using the same199738
JP H09256117 AIron-base soft-magnetic alloy, and thin magnetic element using same—2
JP H1060607 AHigh hardness ferrous soft magnetic alloy—3
JP H1081914 AManufacture of fe-base soft magnetic alloy—1
JP H10306314 AManufacture of soft magnetic alloy—6
JP H1186641 ACable—12
US 6,258,185 B1Methods of forming steel200186
US 6,261,386 B1Nanocrystal dispersed amorphous alloys200136
US 6,270,591 B2Amorphous and nanocrystalline glass-covered wires200172
US 6,773,817 B1Antiabrasion coating200440