Patents
US 7,060,641 B2#793966 Most CitedExpiredUnited States (USPTO)Utility

Diamond-silicon carbide composite

55Forward Citations (#793966 Global)
2.8/yrCitation Velocity (#1074214 Global)
4.14Citation PageRank (#4509008 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Fully dense, diamond-silicon carbide composites are prepared from ball-milled microcrystalline diamond/amorphous silicon powder mixture. The ball-milled powder is sintered (P=5–8 GPa, T=1400K–2300K) to form composites having high fracture toughness. A composite made at 5 GPa/1673K had a measured fracture toughness of 12 MPa·m 1/2 . By contrast, liquid infiltration of silicon into diamond powder at 5 GPa/1673K produces a composite with higher hardness but lower fracture toughness. X-ray diffraction patterns and Raman spectra indicate that amorphous silicon is partially transformed into nanocrystalline silicon at 5 GPa/873K, and nanocrystalline silicon carbide forms at higher temperatures.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 55.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A fully dense diamond-silicon carbide composite made by the method comprising ball-milling a mixture of microcrystalline diamond powder and crystalline silicon to form a ball-milled powder mixture of microcrystalline diamond and amorphous silicon, then sintering the ball-milled powder mixture at a pressure of about 5 GPa to about 8 GPa and a temperature from about 1400K to about 2300K to form a fully dense diamond-silicon carbide composite comprising microcrystalline diamond and nanocrystalline silicon carbide and having a fracture toughness of at least 10 MPa·m 1/2 with minimal graphitizatio

  2. Claim 2Depends on #1

    The composite of claim 1 having a fracture toughness of 12 MPa·m 1/2 .

  3. Claim 3Depends on #1

    The composite of claim 1 , wherein the ball-milled powder is sintered at a pressure of about 5 GPa and a temperature of about 1423K to about 1523K.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 55 total)

PatentTitleYearCitations
US 2007046119 A1Bearing apparatuses, systems including same, and related methods—61
US 8,950,649 B2Apparatus for brazing radial bearings and related methods20152
US 8,651,743 B2Tilting superhard bearing elements in bearing assemblies, apparatuses, and motor assemblies using the same201412
US 2008023231 A1Superabrasive element comprising ultra-dispersed diamond grain structures, structures utilizing same, and methods of manufacture—72
WO 2014/014673 A1Tilting pad bearing assembly—6
US 2008085407 A1Superabrasive elements, methods of manufacturing, and drill bits including same—74
US 7,516,804 B2Polycrystalline diamond element comprising ultra-dispersed diamond grain structures and applications utilizing same200950
US 2011031034 A1Polycrystalline compacts including in-situ nucleated grains, earth-boring tools including such compacts, and methods of forming such compacts and tools—57
CN 101,324,175 BDiamond-silicon carbide combination drill teeth for petroleum probe boring and manufacture method thereof20110
US 8,678,801 B2Injection mold assembly including an injection mold cavity at least partially defined by a polycrystalline diamond material20143
US 2006217258 A1Diamond-silicon carbide composite and method—11
US 8,353,974 B2Superabrasive elements, methods of manufacturing, and drill bits including same20135
US 2011139514 A1Thermally Stable Diamond Bonded Materials and Compacts—12
US 2008206576 A1Superabrasive compact including diamond-silicon carbide composite, methods of fabrication thereof, and applications therefor—135
US 8,727,042 B2Polycrystalline compacts having material disposed in interstitial spaces therein, and cutting elements including such compacts201415

Non-Patent Literature (5)

  • A. Shulzhenko, V. G. Gargin, A. A. Bochechka, G. S. Oleinik, and N. V. Danilenko, "Production, Structure, Properties, The use of Diamond Nanopowders to Strengthen a Diamond-SiC Composite Material," Journal of Superhard Materials, vol. 22, No. 3, pp. 1-13, 2000.
  • A. Witek, B. Palosz, S. Stel'makh, S. Gierlotka, R. Pielaszek, E. Ekimov, V. Filonenko, A. Gavriliuk, and V. Gryaznov, "Sintering of Compacts from Nanocrystalline Diamonds Without Sintering Agent," Mat. Res. Soc. Symp. Proc., vol. 499, pp. 115-120, 1998.
  • E. A. Ekimov, A. G. Gavriliuk, B. Palosz, S. Gierlotka, P. Dluzewski, E. Tatianin, Yu. Kluev, A. M. Naletov, and A. Presz, "High-Pressure, High-Temperature Synthesis of SiC-Diamond Nanocrystalline Ceramics," Appl. Phys. Lett., vol. 77, No. 7, pp. 954-956, Aug. 2000.
  • G. A. Voronin et al., "Diamond-SiC Nanocomposites Sintered From a Mixture of Diamond and Silicon Nanopowders," Diamond and Related Materials, vol. 12, issue 9, pp. 1173-1178, published May 2003.
  • G. A. Voronin, "High Pressure Sintering of Diamond- and CBN-Based Composite Materials by Infiltration: Main Stages and Regularities," V. Bakel Institute for Superhard Materials of the National Academy of Science of Ukraine, pp. 467, no date.