Surface preparation prior to deposition

12Forward Citations (#8586181 Global)
0.6/yrCitation Velocity (#13054367 Global)
1.97Citation PageRank (#14939745 Global)
32Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Methods are provided herein for treating substrate surfaces in preparation for subsequent nucleation-sensitive depositions (e.g., polysilicon or poly-SiGe) and adsorption-driven deposition (e.g. atomic layer deposition or ALD). Prior to depositing, the surface is treated with non-depositing plasma products. The treated surface more readily nucleates polysilicon and poly-SiGe (such as for a gate electrode), or more readily adsorbs ALD reactants (such as for a gate dielectric). The surface treatment provides surface moieties more readily susceptible to a subsequent deposition reaction, or more readily susceptible to further surface treatment prior to deposition. By changing the surface termination of the substrate with a low temperature radical treatment, subsequent deposition is advantageously facilitated without depositing a layer of any appreciable thickness and without significantly affecting the bulk properties of the underlying material. Preferably less than 10 Å of the bulk material incorporates the excited species, which can include fluorine, chlorine and particularly nitrogen excited species.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 12.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of depositing a film on a semiconductor surface in a partially fabricated integrated circuit, the method comprising: exposing the surface to products of a plasma, thereby modifying termination of the semiconductor surface without significantly affecting bulk properties beneath the surface; and after modifying the surface termination, depositing a layer thereover using an atomic layer deposition process; wherein exposing incorporates less than 1 atomic % of the products of the plasma at a depth of greater than about 10 Å from the surface.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the plasma comprises a nitrogen excited species.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the atomic layer deposition comprises depositing an oxide having a higher dielectric constant than silicon nitride.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (32)

PatentTitleYearCitations
US 2,394,930 AFormation of mirrors by thermal evaporation194631
US 3,895,127 AMethod of selectively depositing glass on semiconductor devices197540
US 4,056,642 AMethod of fabricating metal-semiconductor interfaces1977116
US 4,292,343 AMethod of manufacturing semiconductor bodies composed of amorphous silicon198131
US 4,343,830 AMethod for improving the efficiency of solar cells having imperfections198242
US 4,436,761 AMethod for treatment of metal substrate for growth of hydrogen-containing semiconductor film198447
US 4,544,571 AMethod of manufacture of EMI/RFI vapor deposited composite shielding panel198543
JP S60254621 AThin film forming method—11
US 4,645,683 AMethod of manufacturing a semiconductor device198740
US 4,766,006 ALow pressure chemical vapor deposition of metal silicide198861
US 5,135,775 AProcess for plasma-chemical cleaning prior to pvd or pecvd coating199258
US 5,281,546 AMethod of fabricating a thin film transistor using hydrogen plasma treatment of the intrinsic silicon/doped layer interface199469
EP 0,617,461 A2Oxynitride dielectric process for IC manufacture—18
US 5,576,071 AMethod of reducing carbon incorporation into films produced by chemical vapor deposition involving organic precursor compounds199687
US 5,587,205 APlasma processing method and an apparatus for carrying out the same199653
US 5,780,115 AMethods for fabricating electrode structures including oxygen and nitrogen plasma treatments199856
US 5,939,763 AUltrathin oxynitride structure and process for VLSI applications1999220
US 5,950,107 AIn-situ pre-ILD deposition treatment to improve ILD to metal adhesion199936

Non-Patent Literature (2)

  • Kim, H. and R. Reif, Thin Solid Films, vol. 289:192-198 (1996), "In-situ low-temperature (600° C) wafer surface cleaning by electron cyclotron resonance hydrogen plasma . . . ".
  • Ramm J. and E. Beck, Thin Solid Films, vol. 246:158-163 (1994), "Low temperature epitaxial growth by molecular beam epitaxy on hydrogen-plasma-cleaned silicon wafers.".