A semiconductor wafer having a high degree of thinness and exhibiting an enhanced strength state. A layer of tenacious reinforcement material is disposed over a back side of the wafer while in a rough state from backgrinding without prior, conventional polishing or plasma etching of the back side. The thin layer or film of reinforcement material fills grooves, fractures and scratches in the back side of the wafer, enhance the rigidity of the wafer and provide a planar, smooth, back side surface layer. The reinforcement material counteracts internal stresses of the wafer tending to warp, crack and propagate lattice defects in the wafer. The reinforcement material may also be configured to act as a die attach adhesive, may provide an ionic barrier, and may remain as part of the packaging for semiconductor dice singulated from the wafer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for thinning a semiconductor wafer, comprising: providing a semiconductor wafer having a circuitized active surface and a back side surface; securing and supporting the semiconductor wafer in a substantially unwarped state on a fixture; and, while maintaining the semiconductor wafer in the substantially unwarped state: backgrinding the back side surface to a selected thickness; applying material to the back side surface to penetrate recesses in topography thereof and adhere thereto; and hardening the material to a solid state exhibiting a substantially planar exposed surface and bonde

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
JP S59104523 AProduction of infrared-ray detector—7
US 5,164,815 AIntegrated circuit device and method to prevent cracking during surface mount199238
US 5,313,102 AIntegrated circuit device having a polyimide moisture barrier coating199443
US 5,476,566 AMethod for thinning a semiconductor wafer1995192
US 5,583,372 AAdhesion enhanced semiconductor die for mold compound packaging199637
US 6,027,659 APolishing pad conditioning surface having integral conditioning points200083
US 6,184,064 B1Semiconductor die back side surface and method of fabrication2001154
US 6,235,387 B1Semiconductor wafer processing tapes200134
US 6,245,677 B1Backside chemical etching and polishing200161
US 6,258,198 B1Method and apparatus for applying a protecting film to a semiconductor wafer200143
US 6,279,976 B1Wafer handling device having conforming perimeter seal200172
US 6,403,449 B1Method of relieving surface tension on a semiconductor wafer200222
US 6,472,750 B1Process for realizing an intermediate dielectric layer for enhancing the planarity in semiconductor electronic devices200218
US 6,506,681 B2Thin flip—chip method2003155
US 6,534,419 B1Method and apparatus for reducing IC die mass and thickness while improving strength characteristics200322
US 2003096507 A1Backside protection films—29
US 2004029041 A1Novel planarization method for multi-layer lithography processing—73
US 6,727,184 B1Method for coating a thick spin-on-glass layer on a semiconductor structure200418
US 2004110010 A1Reworkable b-stageable adhesive and use in waferlevel underfill—48

Non-Patent Literature (1)

  • Wolf et al., "Silicon Processing for the VLSI Era," vol. 1: Process Technology, Lattice Press, 1986, pp. 238-239.