Abstract

The fuel-barrier polyamide resin of the present invention is a product of the polycondensation of a diamine component comprising 70 mol % or higher of m-xylylenediamine and a dicarboxylic acid component comprising 70 mol % or higher of a mixed dicarboxylic acid which comprises a C 4 to C 20 α,ω-linear aliphatic dicarboxylic acid and at least one dicarboxylic acid selected from the group consisting of isophthalic acid and naphthalenedicarboxylic acid in a molar ratio of 30:70 to 95:5. The polyamide resin is excellent in not only fuel-barrier property and heat resistance, but also moldability and recyclability, and therefore suitably used as a barrier material of fuel containers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A fuel-barrier multilayer molded article comprising a laminated structure of a layer made of a polyamide resin and a high-density polyethylene, wherein the polyamide resin is a polyamide resin produced by the polycondensation of a diamine component comprising 70 mol % or higher of m-xylylenediamine and a dicarboxylic acid component comprising 70 mol % or higher of a mixed dicarboxylic acid which comprises a C 4 to C 20 α,ω-linear aliphatic dicarboxylic acid and at least one dicarboxylic acid selected from the group consisting of isophthalic acid and naphthalenedicarboxylic acid in a molar ra

  2. Claim 2Depends on #1

    The fuel-barrier multilayer molded article according to claim 1 , wherein the polyamide resin contains smectite treated with an organic swelling agent in an amount of 1 to 20% by weight based on a total weight of the polyamide resin and the smectite.