Coated article including titanium oxycarbide and method of making same

8Forward Citations (#12851561 Global)
0.4/yrCitation Velocity (#19672293 Global)
2.27Citation PageRank (#11887864 Global)
21Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A coated article is provided which includes a layer including titanium oxycarbide. In order to form the coated article, a layer of titanium oxide is deposited on a substrate by sputtering or the like. After sputtering of the layer including titanium oxide, an ion beam source(s) is used to implant at least carbon ions into the titanium oxide. When implanting, the carbon ions have sufficient ion energy so as to knock off oxygen (O) from TiO x molecules so as to enable a substantially continuous layer comprising titanium oxycarbide to form near a surface of the previously sputtered layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of making a coated article, the method comprising: providing a glass substrate; sputtering a layer comprising titanium oxide TiO x (where x is from 1 to 3) on the substrate, thereby forming a sputtered layer; and utilizing at least one ion source using anode-cathode voltage of at least about 1,500 V to cause at least carbon ions to be directed toward the sputtered layer comprising titanium oxide so that at least some of the carbon ions are implanted into the sputtered layer to a depth of at least 25 Å below a surface of the sputtered layer, so that a layer comprising titanium oxycarb

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said carbon ions are implanted into the sputtered layer so as to form a substantially continuous layer comprising titanium oxycarbide proximate the surface of the sputtered

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 4,497,700 AMethod of coating a transparent substrate1985132
US 4,693,944 ASurface-coated wear-resistant member of cermet and process for producing same198716
US 5,073,411 AProcess for forming a surface oxidized binding layer on hard substrates19918
US 5,135,808 AAbrasion wear resistant coated substrate product1992241
JP H06158273 AFormation of thin carbide crystal film—4
US 5,569,501 ADiamond-like carbon films from a hydrocarbon helium plasma199662
US 5,637,353 AAbrasion wear resistant coated substrate product1997116
US 5,653,812 AMethod and apparatus for deposition of diamond-like carbon coatings on drills199797
US 5,770,261 AMethod of manufacturing coated cutting tool and coated cutting tool made from199837
US 5,858,477 AMethod for producing recording media having protective overcoats of highly tetrahedral amorphous carbon1999170
US 5,900,342 APhotoconductive element having an outermost layer of a fluorinated diamond-like carbon and method of making the same199974
EP 0,937,013 A1Transparent substrate coated with at least one thin deposit—5
EP 0,997,191 A1Photocatalyst having visible light activity and uses thereof—19
US 6,077,569 AHighly durable and abrasion-resistant dielectric coatings for lenses200067
US 6,261,693 B1Highly tetrahedral amorphous carbon coating on glass2001185
WO 0,159,172 A1Diamond-like carbon film with enhanced adhesion—8
US 6,303,225 B1Hydrophilic coating including DLC on substrate2001197
EP 1,160,353 A1Coated cemented carbide cutting tool member and process for producing the same—26
US 6,334,938 B2Target and process for its production, and method for forming a film having a high refractive index200218
US 6,461,731 B1Solar management coating system including protective DLC2002138
US 6,660,340 B1Diamond-like carbon film with enhanced adhesion200371

Non-Patent Literature (1)

  • International Search Report mailed Mar. 8, 2005.