Patents
US 7,049,003 B2#4894440 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing windshield using ion beam milling of glass substrate(s)

18Forward Citations (#4894440 Global)
0.9/yrCitation Velocity (#7924663 Global)
3.25Citation PageRank (#6651628 Global)
45Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

This invention relates to a method of making a laminated window such as a vehicle windshield. At least one of the two glass substrates of the window is ion beam milled prior to heat treatment and lamination. As a result, defects in the resulting window and/or haze may be reduced.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 45 · Forward citations: 18.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A vehicle windshield comprising: first and second glass substrates laminated to one another via a polymer inclusive interlayer; a low-E coating provided on the first substrate, the low-E coating including from the first glass substrate outwardly at least the following layers: a layer comprising a metal oxide, a contact layer, a layer comprising silver, another contact layer, a layer comprising a metal oxide, another contact layer, another layer comprising silver, another contact layer, and a layer comprising silicon nitride; wherein the first glass substrate is an ion beam milled glass substra

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)

PatentTitleYearCitations
US 8,541,792 B2Method of treating the surface of a soda lime silica glass substrate, surface-treated glass substrate, and device incorporating the same20139
US 2015103398 A1Ir reflective coating compatible to ir sensors—15
US 7,875,945 B2Rear electrode structure for use in photovoltaic device such as CIGS/CIS photovoltaic device and method of making same201131
US 2008308147 A1Rear electrode structure for use in photovoltaic device such as CIGS/CIS photovoltaic device and method of making same—42
US 2008308156 A1Textured rear electrode structure for use in photovoltaic device such as CIGS/CIS solar cell—29
US 2011061730 A1Textured rear electrode structure for use in photovoltaic device such as CIGS/CIS solar cell—5
US 2009020157 A1Rear electrode structure for use in photovoltaic device such as CIGS/CIS photovoltaic device and method of making same—51
WO 2008/156556 A2Rear electrode structure for use in photovoltaic device such as cigs/cis photovoltaic device and method of making same—4
EP 2,280,407 A2Sputtering apparatus including cathode with rotatable targets, and related methods—4
US 8,133,747 B2Textured rear electrode structure for use in photovoltaic device such as CIGS/CIS solar cell20120
WO 2012/050597 A1Method of treating the surface of a soda lime silica glass substrate, surface-treated glass substrate, and device incorporating the same—0
US 8,415,194 B2Rear electrode structure for use in photovoltaic device such as CIGS/CIS photovoltaic device and method of making same201310
US 2011097841 A1Rear electrode structure for use in photovoltaic device such as CIGS/CIS photovoltaic device and method of making same—18
WO 2008/156521 A2Textured rear electrode structure for use in photovoltaic device such as cigs/cis solar cell—2
US 7,846,750 B2Textured rear electrode structure for use in photovoltaic device such as CIGS/CIS solar cell201010

Non-Patent Literature (5)

  • "Highly Tetrahedral, Diamond-Like Amorphous Hydrogenated Carbon Prepared from a Plasma Beam Source", Weiler et al., May 1994, No. 21.
  • "Optical Interference Coatings", Technical Digest 1995, vol. 17, pp. 115-117.
  • "Preparation and Properties of Highly Tetrahedral Hydrogenated Amorphous Carbon", Weiler et al., vol. 53, No. 3, Jan. 1996, pp. 1594-1608.
  • "Surface Hardening of Ceramic and Glass Materials", vol. 36, No. 03, Mar. 1993, p. 291.
  • International Search Report dated Mar. 27, 2003.