Metal/ceramic bonding article and method for producing same

2Forward Citations (#43207948 Global)
0.1/yrCitation Velocity (#45770570 Global)
0.94Citation PageRank (#45679029 Global)
17Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

There is provided a method for producing a metal/ceramic bonding article wherein a metal member 12 is formed so as to have a predetermined shape by printing a resist 14 in a predetermined region on the metal member 12 to etch the metal member 12 after bonding the metal member 12 to a ceramic member 10. In this method, at least one strip-like non-printed portion 16 having a width of, e.g. 0.01 to 0.5 mm, in which the resist is not printed, is provided in a region inwardly spaced from the outer periphery of the resist 14 by a predetermined distance, e.g. 0.01 to 0.5 mm, to control the etch rate in the outer peripheral portion of the metal member 12. Thus, the width and thickness of a fillet is freely changed. For example, a stepped portion (or a stepped portion and fillet) having a width of 0.05 to 0.5 mm and a thickness of 0.005 to 0.25 mm is formed in the outer peripheral portion of the metal member 12.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for producing a metal/ceramic bonding article, said method comprising the steps of: bonding a metal member to a ceramic member; forming a resist on the metal member so that the resist has at least one non-formed portion in which the resist is not formed and which extends along an outer periphery of the resist in a region inwardly spaced from the outer periphery of the resist; and etching an outer peripheral portion of the metal member, wherein at said etching step, said non-formed portion controls an etch rate in the outer peripheral portion of the metal member to form a stepped porti

  2. Claim 2Depends on #1

    A method for producing a metal/ceramic bonding article as set forth in claim 1 , wherein said region is spaced from the outer periphery of the resist by 0.01 to 0.5 mm, and said non-formed portion has a width

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Japanese Patent Laid-Open No. 10-326949 (published on May 26, 1997).