Foil-form soldering metal and method for processing the same
Abstract
The present invention provides a processing method capable of continuously working an Au—Sn soldering metal having a foil form in room temperature. The foil-form soldering metal containing from 10% by weight to 90% by weight of Au and balance comprising Sn is subjected to heat treatment for five minutes to ten hours at 200° C. to 270° C., and subsequently the foil-form soldering metal is slit. Thus, the heat treatment of the Au—Sn soldering metal before slitting enables continuous slitting of the Au—Sn foil-form soldering metal in room temperature and facilitates the production of a ribbon-form soldering metal.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 8.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for processing a foil-form soldering metal containing from 10% by weight to 90% by weight of Au and balance comprising Sn, comprising: subjecting the foil-form soldering metal to heat treatment for five minutes to ten hours at 200° C. to 270° C.; and subsequently processing the foil-form soldering metal.
- Claim 2Depends on #1
The method for processing a foil-form soldering metal according to claim 1 , wherein the processing after heat treatment is slitting, rolling or blanking.
- Claim 3Depends on #2
The method for processing a foil-form soldering metal according to claim 2 , comprising the step of rolling after heat treatment before slitting or blanking.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗