Silicon single crystal wafer fabricating method and silicon single crystal wafer

5Forward Citations (#19078388 Global)
0.2/yrCitation Velocity (#28168429 Global)
3.20Citation PageRank (#6823307 Global)
15Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

At the time of fabricating a silicon single crystal wafer from a nitrogen-doped silicon single crystal grown according to the Czochralski method, a silicon single crystal wafer covered with a region in which an oxygen precipitation bulk micro defect and an oxidation induced stacking fault mixedly exist is subjected to heat treatment at a temperature of 1100 to 1300° C. in a reducing gas or inert gas atmosphere. In such a manner, a method of fabricating a high-quality silicon single crystal wafer and a silicon single crystal wafer in which no grown-in crystal defects exist in the whole surface and oxygen precipitation bulk micro defects (BMD) are formed at a sufficiently high density to display the IG effect on the inner side can be provided. The single crystal wafer can be suitably used to form an operation region of a semiconductor device.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A silicon single crystal wafer fabricating method of fabricating a silicon single crystal wafer from a nitrogen-doped silicon single crystal grown according to the Czochralski method, wherein a silicon single crystal wafer covered with a region in which an oxygen precipitation bulk micro defect and an oxidation induced stacking fault mixedly exist is subjected to heat treatment at a temperature of 1100 to 1300° C. in a reducing gas or inert gas atmosphere.

  2. Claim 2Depends on #1

    The silicon single crystal wafer fabricating method according to claim 1 , wherein at the time of growing said nitrogen-doped silicon single crystal, a V/G value as a ratio between a pulling rate V (mm/min) of a single crystal and a temperature gradient G (° C./mm) in the axial direction of the single crystal where a region in which both the oxygen precipitation bulk micro defect and an oxidation induced stackin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (15)

PatentTitleYearCitations
JP H08330316 ASilicon single crystal wafer and its production—120
US 6,077,343 ASilicon single crystal wafer having few defects wherein nitrogen is doped and a method for producing it200030
JP 2000272997 AGrowth of silicon single crystal and silicon wafer using the same and estimation of amount of nitrogen doped in the silicon wafer—10
US 6,180,220 B1Ideal Oxygen precipitating silicon wafers and oxygen out-diffusion-less process therefor200156
WO 0,127,362 A1Silicon single-crystal wafer for epitaxial wafer, epitaxial wafer, methods for producing them, and evaluating method—20
US 6,261,361 B1Silicon single crystal wafer having few defects wherein nitrogen is doped and a method for producing it200130
WO 0,155,485 A1Silicon wafer, method for determining condition under which silicon single crystal is produced, and method for producing silicon wafer—9
WO 02,103,091 A1SILICON SINGLE CRYSTAL WAFER HAVING VOID DENUDED ZONE ON THE SUFRACE AND DIAMETER OF AVOBE 300 mm AND ITS PRODUCTION METHOD—3
US 6,503,594 B2Silicon wafers having controlled distribution of defects and slip200326
US 2003015131 A1Silicon Wafer, Method for Determining Production Conditions of Silicon Single Crystal and Method for Producing Silicon Wafer—15
US 6,517,632 B2Method of fabricating a single crystal ingot and method of fabricating a silicon wafer200321
US 6,548,035 B1Silicon single crystal wafer for epitaxial wafer, epitaxial wafer, and methods for producing the same and evaluating the same200330
US 6,599,360 B2Silicon wafer, method for determining production conditions of silicon single crystal and method for producing silicon wafer200313
US 2003172865 A1Silicon single crystal wafer having void denuded zone on the surface and diameter of above 300mm and its production method—10
US 6,666,915 B2Method for the preparation of an epitaxial silicon wafer with intrinsic gettering200318

Non-Patent Literature (2)

  • M. Iida et al., "Effects of Light Element Impurities on the Formation of Grown-in Defects Free Region of Czochralski Silicon Single Crystal," Defects in Silicon 99-1:499-510, The Electrochemical Society, Inc., Pennington, NJ.
  • M. Tamatsuka et al., "High Performance Silicon Wafer With Wide Grown-in Void Free Zone and High Density Internal Gettering Site Achieved Via Rapid Crystal Growth With Nitrogen Doping and High Temperature Hydrogen and/or Argon Annealing," Defects in Silicon 99-1:456-467, The Electrochemical Society,