Patents
US 7,033,939 B2#50600317 Most CitedExpiredUnited States (USPTO)Utility

Chemistry for chemical vapor deposition of titanium containing films

1Forward Citations (#50600317 Global)
0.1/yrCitation Velocity (#54293879 Global)
0.85Citation PageRank (#50600317 Global)
25Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Titanium-containing films exhibiting excellent uniformity and step coverage are deposited on semiconductor wafers in a cold wall reactor which has been modified to discharge plasma into the reaction chamber. Titanium tetrabromide, titanium tetraiodide, or titanium tetrachloride, along with hydrogen, enter the reaction chamber and come in contact with a heated semiconductor wafer, thereby depositing a thin titanium-containing film on the wafer's surface. Step coverage and deposition rate are enhanced by the presence of the plasma. The use of titanium tetrabromide or titanium tetraiodide instead of titanium tetrachloride also increases the deposition rate and allows for a lower reaction temperature. Titanium silicide and titanium nitride can also be deposited by this method by varying the gas incorporated with the titanium precursors.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for disposing a titanium-containing film on a substrate, the method comprising the acts of: disposing a substrate inside a reaction chamber; bringing the substrate to a given temperature; introducing a titanium source gas into the reaction chamber; introducing a reactant gas into the reaction chamber; generating a plasma above the substrate; and applying a voltage directly to the substrate to deposit a titanium-containing film on the substrate, where the voltage is not applied through an intermediary structure.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein a deposition pressure between 0.2 and 2 Torr is maintained in the reaction chamber.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the reaction chamber comprises a hot wall reaction chamber.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (25)

PatentTitleYearCitations
US 4,786,352 AApparatus for in-situ chamber cleaning1988219
US 4,897,709 ATitanium nitride film in contact hole with large aspect ratio1990147
US 5,399,379 ALow-pressure chemical vapor deposition process for depositing high-density, highly-conformal titanium nitride films of low bulk resistivity199595
US 5,431,958 AMetalorganic chemical vapor deposition of ferroelectric thin films199575
US 5,455,138 AProcess for forming deposited film for light-receiving member, light-receiving member produced by the process, deposited film forming apparatus, and method for cleaning deposited film forming apparatus199546
US 5,508,066 AMethod for forming a thin film199633
US 5,510,151 AContinuous film-forming process using microwave energy in a moving substrate web functioning as a substrate and plasma generating space199638
US 5,567,243 AApparatus for producing thin films by low temperature plasma-enhanced chemical vapor deposition using a rotating susceptor reactor1996162
US 5,595,784 ATitanium nitride and multilayers formed by chemical vapor deposition of titanium halides1997111
US 5,647,953 APlasma cleaning method for removing residues in a plasma process chamber1997165
US 5,723,382 AMethod of making a low-resistance contact to silicon having a titanium silicide interface, an amorphous titanium nitride barrier layer and a conductive plug199867
US 5,747,116 AMethod of forming an electrical contact to a silicon substrate199869
US 5,834,371 AMethod and apparatus for preparing and metallizing high aspect ratio silicon semiconductor device contacts to reduce the resistivity thereof1998102
US 5,888,906 APlasmaless dry contact cleaning method using interhalogen compounds199965
US 5,891,349 APlasma enhanced CVD apparatus and process, and dry etching apparatus and process199977
US 5,976,976 AMethod of forming titanium silicide and titanium by chemical vapor deposition199956
US 6,040,021 APlasma CVD process for metal films and metal nitride films200050
US 6,090,709 AMethods for chemical vapor deposition and preparation of conformal titanium-based films200049
US 6,168,837 B1Chemical vapor depositions process for depositing titanium silicide films from an organometallic compound20019
US 6,176,936 B1In-situ chamber cleaning method of CVD apparatus200117
US 6,204,192 B1Plasma cleaning process for openings formed in at least one low dielectric constant insulation layer over copper metallization in integrated circuit structures2001145
US 6,214,739 B1Method of metal etching with in-situ plasma cleaning200117
US 6,218,300 B1Method and apparatus for forming a titanium doped tantalum pentaoxide dielectric layer using CVD200114
US 6,294,466 B1HDP-CVD apparatus and process for depositing titanium films for semiconductor devices200142
US 6,534,133 B1Methodology for in-situ doping of aluminum coatings200345