Abstract

Disclosed are a light absorbent agent polymer for organic anti-reflective coating which can prevent diffused reflection of lower film layer or substrate and reduce standing waves caused by variation of thickness of the photoresist itself, thereby, increasing uniformity of the photoresist pattern, in a process for forming ultra-fine patterns of photoresist for photolithography by using 193 nm ArF among processes for manufacturing semiconductor device, and its preparation method. Also, the present invention discloses an organic anti-reflective coating composition comprising the light absorbent agent polymer for the organic anti-reflective coating and a pattern formation process using the coating composition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 17.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A light absorbent agent polymer for organic anti-reflective coating represented by the following formula I: wherein a and b represent the mole percent of respective monomers and a:b=5 to 95:5 to 95.

  2. Claim 2Independent Claim

    A method for preparing a light absorbent agent polymer for organic anti-reflective coating, comprising the steps of: dissolving a maleic anhydride and 1,4-dihydro- 1,4-methanonaphthalene-5,8-diol diacetate in an organic solvent; adding a polymerization initiator to the dissolved material; and producing a polymer represented by the following formula I by polymerizing the dissolved material under vacuum condition, at 60 to 70° C. for 2 to 6 hours: wherein a and b represent the mole percent of respective monomers and a:b=5 to 95:5 to 95.

  3. Claim 3Depends on #2

    The method according to claim 2 , wherein the organic solvent

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗