US 7,022,378 B2#5664672 Most CitedExpiredUnited States (USPTO)Utility

Nitrogen passivation of interface states in SiO2/SiC structures

16Forward Citations (#5664672 Global)
0.8/yrCitation Velocity (#9114114 Global)
3.55Citation PageRank (#5776652 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A nitrided oxide layer on a silicon carbide layer is processed by annealing the nitrided oxide layer in a substantially oxygen-free nitrogen containing ambient. The anneal may be carried out at a temperature of greater than about 900° C., for example, a temperature of about 1100° C., a temperature of about 1200° C. or a temperature of about 1300° C. Annealing the nitrided oxide layer may be carried out at a pressure of less than about 1 atmosphere, for example, at a pressure of from about 0.01 to about 1 atm or, in particular, at a pressure of about 0.2 atm. The nitrided oxide layer may be an oxide layer that is grown in a N 2 O and/or NO containing ambient, that is annealed in a N 2 O and/or NO containing ambient or that is grown and annealed in a N 2 O and/or NO containing ambient.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 16.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of processing a nitrided oxide layer on a silicon carbide layer, the method comprising: annealing the nitrided oxide layer in a substantially oxygen-free nitrogen containing ambient, wherein the substantially oxygen-free nitrogen containing ambient comprises a NH 3 containing ambient, wherein the substantially oxygen-free nitrogen containing ambient comprises NH 3 and SiH 4 .

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the SiH 4 and NH 3 are provided in a reaction chamber containing the nitrided oxide layer such that the SiH 4 and NH 3 are not mixed until a region of the reaction chamber proximate the nitrided oxide layer.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the nitrided oxide layer comprises a thermally grown oxide layer.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 16 total)

PatentTitleYearCitations
US 7,820,558 B2Semiconductor device and method of producing the semiconductor device20104
US 7,381,268 B2Apparatus for production of crystal of group III element nitride and process for producing crystal of group III element nitride200811
US 2013034941 A1Forming sic mosfets with high channel mobility by treating the oxide interface with cesium ions—18
US 2008191217 A1Process for forming an interface between silicon carbide and silicon oxide with low density of states—4
US 2011095304 A1Process for forming an interface between silicon carbide and silicon oxide with low density of states—2
US 8,183,573 B2Process for forming an interface between silicon carbide and silicon oxide with low density of states20122
EP 2,740,148 A4Forming sic mosfets with high channel mobility by treating the oxide interface with cesium ions—0
US 8,765,617 B2Method of manufacturing semiconductor device20142
US 7,754,012 B2Apparatus for production of crystal of group III element nitride and process for producing crystal of group III element nitride20106
US 7,888,256 B2Process for forming an interface between silicon carbide and silicon oxide with low density of states20111
US 2008213158 A1Apparatus for production of crystal of group III element nitride and process for producing crystal of group III element nitride—1
US 2012231618 A1Method of manufacturing semiconductor device—11
US 2008135954 A1Semiconductor device and method of producing the semiconductor device—29
WO 2013/019334 A1Forming sic mosfets with high channel mobility by treating the oxide interface with cesium ions—0
WO 2013/061702 A1Semiconductor device manufacturing method—0

Non-Patent Literature (5)

  • A.K. Agarwal, S. Seshadri, and L. B. Rowland, "Temperature Dependence of Fowler-Nordheim Current in 6H-and 4-H-SiC MOS Capacitors." IEEE Electron Device Letters, vol. 18, No. 12, Dec. 19997, pp. 592-594.
  • Agarwal et al. "1.1 kV 4H-SiC Power UMOSFET's," IEEE Electron Device Letters, vol. 18, No. 12, Dec. 1997, pp. 586-588.
  • Agarwal et al. "1400 V 4H-SiC Power MOSFET's," Materials Science Forum vols. 264-268, pp. 989-992, 1998.
  • Agarwal et al. "A Critical Look at the Performance Advantages and Limitations of 4H-SiC Power UMOSFET Structures," 1996 IEEE ISPSD and IC's Proc., May 20-23, 1996, pp. 119-122.
  • Agarwal et al. "Investigation of Lateral RESURF, 6H-SiC MOSFETs," Materials Science Forum, vols. 338-342, (2000) pp. 1307-1310.