A method of depositing a low dielectric constant film on a substrate and post-treating the low dielectric constant film is provided. The post-treatment includes rapidly heating the low dielectric constant film to a desired high temperature and then rapidly cooling the low dielectric constant film such that the low dielectric constant film is exposed to the desired high temperature for about five seconds or less. In one aspect, the post-treatment also includes exposing the low dielectric constant film to an electron beam treatment and/or UV radiation.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 36 · Forward citations: 13.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of processing a substrate, comprising: depositing a low dielectric constant film comprising silicon and carbon on a substrate in the presence of RF power; and post-treating the depositing low dielectric constant film by a process comprising: heating the low dielectric constant film to a desired temperature of at least about 600° C. at a rate of at least about 10° C./sec, wherein the low dielectric constant film is maintained at the desired temperature for about five seconds or less; and then cooling the low dielectric constant film at a rate of at least about 10° C./sec.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the post-treating is performed under conditions sufficient to lower the dielectric constant of the low dielectric constant film.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the low dielectric constant film is heated at a rate between about

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (36)

PatentTitleYearCitations
US 5,003,178 ALarge-area uniform electron source1991238
US 6,025,279 AMethod of reducing nitride and oxide peeling after planarization using an anneal200033
US 6,030,904 AStabilization of low-k carbon-based dielectrics200040
US 6,033,999 AMethod of solving contact oblique problems of an ILD layer using a rapid thermal anneal20004
US 6,080,526 AIntegration of low-k polymers into interlevel dielectrics using controlled electron-beam radiation2000110
US 6,133,086 AFabrication method of a tantalum pentoxide dielectric layer for a DRAM capacitor200024
US 2001004479 A1Plasma processes for depositing low dielectric constant films—48
WO 0,148,805 A1Method for curing spin-on dielectric films utilizing electron beam radiation—6
US 6,303,524 B1High temperature short time curing of low dielectric constant materials using rapid thermal processing techniques200176
US 6,383,951 B1Low dielectric constant material for integrated circuit fabrication200263
US 2002105084 A1Low dielectric constant material for integrated circuit fabrication—18
US 2002110934 A1Rapid- temperature pulsing anneal method at low temperature for fabricating layered superlattice materials and making electronic devices including same—18
US 6,437,406 B1Super-halo formation in FETs200241
US 6,444,136 B1Fabrication of improved low-k dielectric structures200230
US 2002162500 A1Deposition of tungsten silicide films—17
US 6,500,740 B1Process for fabricating semiconductor devices in which the distribution of dopants is controlled20023
US 2003054115 A1Ultraviolet curing process for porous low-K materials—122

Non-Patent Literature (5)

  • PCT International Search Report for PCT/US2005/002927, dated Apr. 19, 2005. (AMAT/8856.PC)
  • U. S. Appl. No. 10/773,060, filed Feb. 4, 2004 (AMAT/7034.P1).
  • U.S. Appl. No. 10/461,638, filed Jun. 12, 2003 (AMAT/8435).
  • U.S. Appl. No. 10/642,081, filed Aug. 14, 2003 (AMAT/8435.02).
  • U.S. Appl. No. 10/668,682, filed Sep. 22, 2003 (AMAT/7916).