Melt spun thermoplastic polyurethanes useful as textile fibers
Abstract
Melt spun thermoplastic polyurethane polymers useful as textile fibers and having good tenacity and recovery and substantially no gelation are disclosed. The polymers are prepared by a three-step polymerization process including: preparation of “hard” segment oligomer, preparation of “soft” segment oligomer and final reaction of “hard” segment with “soft” segment in a twin-screw reaction extruder to obtain a final polyurethane product having relatively uniform distances between the “hard” segments. The “soft” segment oligomer comprises blocks of polymeric glycol (poly) urethanes end capped with isocyanate groups. The “hard” segment oligomer comprises blocks of low molecular weight C 2 –C 6 glycol (poly) urethanes.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 4.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A composition useful in preparing melt spun textile fibers comprising a polyurethane polymer consisting of the reaction product of monomers consisting of at least one diisocyanate monomer and at least two diol monomers, a first diol monomer which is a member selected from the group consisting of a polyether diol, a polyester diol, hydroxyl terminated polyether/polyester glycols and mixtures thereof; and a second diol monomer having a molecular weight of about 62 to about 118, said polyurethane having a molecular weight of about 200,000 and above, a tenacity of about 0.6 gm/denier and above, an
- Claim 2Depends on #1
A composition according to claim 1 wherein the at least one diisocyanate monomer is a member selected from th
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗