Patents
US 7,015,294 B2#8580457 Most CitedExpiredUnited States (USPTO)Utility

Acrylate polymers based on tert-butyl acrylate and/or tert-butyl methacrylate

12Forward Citations (#8580457 Global)
0.6/yrCitation Velocity (#13052658 Global)
1.98Citation PageRank (#14777493 Global)
6Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention relates to acrylate polymers comprising a K-value ranging from 10 to 60, which can be obtained by the radical polymerization of: 30 to 99 wt. % of tert-butyl acrylate and/or tert-butyl methacrylate designated as monomer A; 1 to 28 wt. % of acrylic acid and/or methacrylic acid designated as monomer B, and; 0 to 60 wt. % of a radically copolymerizable monomer or of a radically copolymerizable monomer mixture designated as monomer C, whereby at least one of monomers C yields a homopolymer with a glass-transition temperature lower than 30° C., with the provision that the wt. %'s total 100. The radical polymerization is carried out in the presence of alkane thiols with a C chain length of C 14 to C 22. The invention also relates to acrylate polymers comprising a K-value ranging from 10 to 60, which can be obtained by the radical polymerization of: 30 to 99 wt. % of tert-butyl acrylate and/or tert-butyl methacrylate designated as monomer A; 1 to 28 wt. % of acrylic acid and/or methacrylic acid designated as monomer B, and; 0 to 60 wt. % of a radically copolymerizable monomer or of a radically copolymerizable monomer mixture designated as monomer C, whereby at least one

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 12.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An acrylate polymer with a K value of from 10 to 60, obtained by free-radical polymerization of 30 to 99% by weight of tert-butyl acrylate and/or tert-butyl methacrylate as monomer A, 1 to 28% by weight of acrylic acid and/or methacrylic acid as monomer B and 0 to 60% by weight of a free-radically copolymerizable monomer or a free-radically copolymerizable monomer mixture as monomer C, where at least one of the monomers C produces a homopolymer with a glass transition temperature of less than 30° C., with the proviso that the % by weight add up to 100, in the presence of alkanethiols with a ca

  2. Claim 2Depends on #1

    An acrylate polymer as claimed in claim 1 , wherein linear alkanethiols are used.

  3. Claim 3Independent Claim

    An acrylat

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗