Abstract

This invention relates to a polymer precursor dispersion for use in making a polymer that is a solid at room temperature and further relates to a method of making same where the dispersion comprises a polymer precursor comprising an addition monomer, a condensation monomer, a prepolymer, or a polymer modifier and 0.01 to 50 weight percent of a micropulp having a volume average length of from 0.01 to 100 micrometers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A polymer precursor dispersion for use in making a polymer that is a solid at room temperature, comprising: a polymer precursor comprising an addition monomer, a condensation monomer, a prepolymer, or a polymer modifier; and a micropulp having a volume average length of from 0.01 to 50 micrometers, the micropulp comprising 0.01 to 50 weight percent of the dispersion.

  2. Claim 2Depends on #1

    The polymer precursor dispersion of claim 1 , wherein said polymer precursor has a viscosity of less than 10,000 centipoise at room temperature.

  3. Claim 3Depends on #1

    The polymer precursor dispersion of claim 1 , wherein the polymer precursor further comprises a solvent.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗