Abstract

A semiconductor device having high operating performance and reliability, and a manufacturing method thereof are provided. An LDD region 207 provided in an n-channel TFT 302 forming a driving circuit enhances the tolerance for hot carrier injection. LDD regions 217–220 provided in an n-channel TFT (pixel TFT) 304 forming a pixel portion greatly contribute to the decrease in the OFF current value. Here, the LDD region of the n-channel TFT of the driving circuit is formed such that the concentration of the n-type impurity element becomes higher as the distance from an adjoining drain region decreases.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 41 · Forward citations: 13.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device comprising: forming a crystalline semiconductor layer over an insulating substrate; forming a gate insulating film on the crystalline semiconductor layer; forming a conductive film on the gate insulating film; and etching the conductive film so as to form a gate electrode having a tapered cross section by using an inductively coupled plasma chamber having multispiral coils.

  2. Claim 2Depends on #1

    A method of manufacturing a semiconductor device according to claim 1 , wherein the gate electrode comprises at least one selected from the group consisting of tantalum, chromium, tungsten, and silicon having conductivity.

  3. Claim 3Depends on #1

    A method of manufacturing a semiconductor device according to claim 1 , wherein a taper angle of the gate electrode is between 3 and 40°.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • 1996, J. Mater. Chem. 6(4), "Thresholdless Antiferroelectricity in liquid crystals and its application to displays," by S. Inui et al., pp. 671-673.
  • 1997 SID Digest, 841, "A Full-Color Thresholdless Antiferroelectric LCD Exhibiting Wide Viewing Angle With Fast Response Time" by T. Yoshida et al., pp. 841-844.
  • 1998 SID, "Characteristics and Driving Scheme of Polymer-Stabilized Monostable FLCD Exhibiting Fast Response Time and High Contrast Ratio with Gray-Scale Capability," by H. Furue et al., pp. 782-785.
  • Inventors: Shunpei Yamazaki et al., "Semiconductor Device and Method for Fabricating the Same", Filing Date: Apr. 7, 2000, Specifications, Drawings and Pending Claims for U.S. Appl. No. 09/544,801.
  • M. Hatano, H. Akimoto, T. Sakai, IEDM 97 Technical Digest, pp. 523-526, 1997.