US 7,015,113 B2#45088147 Most CitedExpiredUnited States (USPTO)Utility

Methods of forming trench isolation regions

2Forward Citations (#45088147 Global)
0.1/yrCitation Velocity (#45874923 Global)
0.88Citation PageRank (#49239139 Global)
13Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention includes methods of forming trench isolation regions. In one implementation, a masking material is formed over a semiconductor substrate. The masking material comprises at least one of tungsten, titanium nitride and amorphous carbon. An opening is formed through the masking material and into the semiconductor substrate effective to form an isolation trench within semiconductive material of the semiconductor substrate. A trench isolation material is formed within the isolation trench and over the masking material outside of the trench effective to overfill the isolation trench. The trench isolation material is polished at least to an outermost surface of the at least one of tungsten, titanium nitride and amorphous carbon of the masking material. The at least one of tungsten, titanium nitride and amorphous carbon is/are etched from the substrate. Other implementations and aspects are contemplated.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of forming a trench isolation region comprising: forming a masking material over a semiconductor substrate; the masking material comprising at least one of tungsten, titanium nitride and amorphous carbon; forming an opening through the masking material and into the semiconductor substrate effective to form an isolation trench within semiconductive material of the semiconductor substrate; forming trench isolation material within the isolation trench and over the masking material outside of the trench effective to overfill the isolation trench; polishing the trench isolation material at

  2. Claim 2Depends on #1

    The method of claim 1 wherein the masking materia

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • D. F. Franceschini et al., Internal stress reduction by nitrogen incorporation in hard amorphous carbon thin films, Appl. Phys. Lett., vol. 60, No. 29, pp. 3229-3231 (Jun. 29, 1992).