Use of selective oxidation to form asymmetrical oxide features during the manufacture of a semiconductor device

3Forward Citations (#33562145 Global)
0.1/yrCitation Velocity (#38825369 Global)
1.02Citation PageRank (#40224754 Global)
14Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A sidewall oxidation process for use during the formation of a transistor such as a flash memory cell allows for improved control of a gate oxide profile. The method comprises doping transistor source and drain regions to different doping levels, then performing a transistor sidewall oxidation using a particular process to modify the gate oxide thickness. The oxide forms at a faster rate along the source sidewall than along the drain sidewall. By using ranges within the oxidation environment described, a source side gate oxide having a variable and selectable thickness may be formed, while forming a drain-side oxide which has a single thickness where a thinner layer is desirable. This leads to improved optimization of key competing requirements of a flash memory cell, such as program and erase performance, while maintaining sufficient long-term data retention. The process may allow improved cell scalability, shortened design time, and decreased manufacturing costs.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method used during the formation of a semiconductor device comprising: implanting a first region of a semiconductor material with a dopant to a first concentration and implanting a second region of the semiconductor material with the dopant to a second concentration, wherein the first concentration is greater than the second concentration; and exposing the first and second regions of the semiconductor material to an oxidizing ambient comprising: a partial pressure of steam, wherein the partial pressure of steam is proportional to an oxidation ratio of the first region to the second region, a