Iron based sintered body excellent in enveloped casting property in light metal alloy and method for producing the same
Abstract
The object of the invention is to provide an iron based sintered body suitable for being enveloped in light metal alloy such as an aluminum alloy by casting, and a method for producing the same. A mixed powder is prepared by mixing an iron based powder, a copper powder and a graphite powder blended so that the Cu content and the C content are 5 to 40% by mass and 0.5 to 2.5% by mass, respectively, in the mixed powder. A lubricant powder and a fine particle powder for improving machinability may be further added in the mixed powder. Then, the mixed powder is filled into a mold formed to a green compact, and is sintered into a sintered body so that the sintered body has a desired average thermal expansion coefficient. The surface of the sintered body may be adjusted to have a surface roughness Rz of 10 to 100 μm optionally by applying a shot blast treatment or by a shot blast treatment and an additional steam treatment. This process permits the sintered body to be enhanced in an adhesive property and bonding strength while being improved in enveloping casting property when the sintered body is enveloped in the light metal alloy by casting. A martesitic stainless steel powder or ferri
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 10.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
An iron based sintered body which is enveloped in a cast light metal alloy member, having a composition comprising, in % by mass, 0.5 to 2.5% of C, 5 to 40% of Cu, and the balance being Fe and inevitable impurities, a structure containing pores, said pores being isolated or partially connected to each other, wherein the value defined by [(the volume of fully connected pores)/(the total volume of pores)×100(%)] is 50 or less, and the volume ratio of the pores relative to a total volume of the sintered body is 13–35% by volume, and free Cu phases dispersed in a matrix, an average thermal expansi
- Claim 2Depends on #1
The iron based sintered body according to claim 1 , wherein the surface is subjected to a shot blast treatment.
- Claim 3Independent Claim
The iron based si
Technical Overview & Description