Patents
US 7,014,571 B2#4347889 Most CitedExpiredUnited States (USPTO)Utility

High density alloy for improved mass properties of an article

20Forward Citations (#4347889 Global)
1.0/yrCitation Velocity (#6528092 Global)
2.00Citation PageRank (#14548442 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention is a nickel-tungsten-chromium alloy for an article of manufacture such as a portion of a golf club head ( 20 ). The nickel-tungsten-chromium alloy preferably has a density ranging from 9.0 g/cm 3 to 10.5 g/cm 3 , and a Rockwell Hardness ranging from 50 to 92. The nickel-tungsten-chromium alloy is capable of being investment cast to form the article of manufacture.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 20.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An iron golf club head comprising: a body composed of a castable nickel-tungsten-chromium alloy comprising 35 to 50 weight percent nickel, 30 to 35 weight percent tungsten and 20 to 30 weight percent chromium and 1 weight percent silicon, the nickel-tungsten-chromium alloy having a density ranging from 9.0 g/cm 3 to 10.5 g/cm 3 , and a Rockwell Hardness ranging from 50 to 92.

  2. Claim 2Depends on #1

    The iron golf club head according to claim 1 wherein the nickel-tungsten alloy has a density ranging from 9.2 g/cm 3 to 10.0 g/cm 3 .

  3. Claim 3Depends on #1

    The iron golf club head according to claim 1 wherein the nickel-tungsten alloy has a Rockwell Hardness ranging from 80 to 91.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗