Metallic strain-absorbing layer for improved fatigue resistance of solder-attached devices

10Forward Citations (#9978928 Global)
0.5/yrCitation Velocity (#15205967 Global)
2.93Citation PageRank (#7854369 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An integrated circuit chip 501 has a plurality of contact pads (FIG. 5 B) to be connected by reflow attachment 510 to outside parts. The chip comprises a deposited layer 505 of nickel/titanium alloy on each of the pads; the alloy has a composition and crystalline structure operable in reversible phase transitions under thermomechanical stress, whereby mechanical strain is absorbed by the alloy layer. Preferably, the alloy has between 55.0 and 56.0 weight % nickel, between 44.0 and 45.0 weight % titanium, and a thickness in the range from 0.3 to 6.0 μm, recrystallized after deposition in a temperature range from 450 to 600° C. for a time period between 4 and 6 min. A layer 506 of solderable metal is on the alloy, operable as diffusion barrier after reflow attachment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 10.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating integrated circuit chips having a plurality of contact pads to be connected by reflow attachment to outside parts, comprising the steps of: depositing a layer of nickel/titanium alloy composed of 55.5 ±0.5 weight % nickel and 44.5±0.5 weight % titanium in the thickness range of 0.3 to 6.0 μm; recrystalling said alloy layer at 500° C. for about 5 mm, creating a crystalline structure operable in reversible phase transitions under thermo-mechanical stress, whereby mechanical strain is absorbed by said alloy layer; depositing a layer of solderable metal on said alloy; and p

  2. Claim 2Depends on #1

    The method according to claim 1 wherein said step of depositing is a DC sputter technique at about 160 W/in 2 for about 1 hour.

  3. Claim 3Depends on #1

    The method according to claim 1 wherein said solderable metal is nickel, deposited by a