US 7,011,978 B2#24092695 Most CitedExpiredUnited States (USPTO)Utility

Methods of forming capacitor constructions comprising perovskite-type dielectric materials with different amount of crystallinity regions

4Forward Citations (#24092695 Global)
0.2/yrCitation Velocity (#32733682 Global)
1.49Citation PageRank (#23169144 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention includes a capacitor construction. A capacitor electrode has a perovskite-type dielectric material thereover. The perovskite-type dielectric material has an edge region proximate the electrode, and a portion further from the electrode than the edge region. The portion has a different amount of crystallinity than the edge region. The invention also includes a method of forming a capacitor construction. A capacitor electrode is provided, and a perovskite-type dielectric material is chemical vapor deposited over the first capacitor electrode. The depositing includes flowing at least one metal organic precursor into a reaction chamber and forming a component of the perovskite-type dielectric material from the precursor. The precursor is exposed to different oxidizing conditions during formation of the perovskite-type dielectric material so that a first region of the dielectric material has more amorphous character than a second region of the dielectric material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a capacitor construction, comprising: providing a first capacitor electrode; forming a perovskite-type dielectric material over the first capacitor electrode, the perovskite-type dielectric material having a first edge region proximate the first electrode and a portion further from the first electrode than the first edge region, the perovskite-type dielectric material having a common chemical composition within the first edge region and said portion, said portion having a different amount of crystallinity than the first edge region; and while the first edge region and the p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,105,810 AChemical vapor deposition methods of depositing zinc boro-silicated glasses197865
US 4,261,698 ATrace oxygen detector198166
EP 0,030,798 A1Low temperature process for depositing oxide layers by photochemical vapor deposition—36
US 4,691,662 ADual plasma microwave apparatus and method for treating a surface1987109
GB 2,194,555 AMethod of manufacturing thin compound oxide film and apparatus for manufacturing thin oxide film—24
EP 0,306,069 A2A method of forming an oxide layer on a substrate—28
EP 0,388,947 A1Sprayhead for a spray container for dispensing foam—9
JP H02250970 AMethod and device for chemical vapor phase growth of tantalum oxide film—9
US 5,006,363 APlasma assited MO-CVD of perooskite dalectric films199151
JP H0424922 AForming method for high permittivity thin film and forming apparatus thereof—17
EP 0,474,140 A1Process of forming capacitive insulating film—26
JP H04115533 AManufacture of semiconductor element and thermal cvd device—16
JP H04180566 AThin film forming device—18
US 5,164,363 AMethod for vapor-phase growth of a superconducting oxide thin film199246
US 5,183,510 AApparatus and process for chemical vapor deposition199367
US 5,254,505 AProcess of forming capacitive insulating film199358
US 5,256,455 AMethod of forming film of tantalum oxide by plasma chemical vapor deposition199338
US 5,261,961 ADevice for forming deposited film199357
US 5,270,241 AOptimized container stacked capacitor DRAM cell utilizing sacrificial oxide deposition and chemical mechanical polishing1993232
US 5,312,783 AProcess for the preparation of a high dielectric thin film using ECR plasma CVD199448
US 5,392,189 ACapacitor compatible with high dielectric constant materials having two independent insulative layers and the method for forming same1995333
US 5,395,771 AGraded implantation of oxygen and/or nitrogen constituents to define buried isolation region in semiconductor devices199550
US 5,459,635 ALaminated thin film capacitor and method for producing the same199547
US 5,468,687 AMethod of making TA2 O5 thin film by low temperature ozone plasma annealing (oxidation)1995127
US 5,470,398 ADielectric thin film and method of manufacturing same199550
JP H0860347 AMethod for depositing dielectric thin film—19

Non-Patent Literature (5)

  • Aoyama et al., "Leakage Current Mechanism of Amorphous and Polycrystalline Ta<SUB>1</SUB>O<SUB>5 </SUB>Film Grown by chemical Vapor Deposition," 1995, pp. 977-983.
  • Aoyama et al., “Leakage Current Mechanism of Amorphous and Polycrystalline Ta1O5 Film Grown by chemical Vapor Deposition,” 1995, pp. 977-983.
  • Arai T., et al.: "Preparation of SrTiO<SUB>3 </SUB>Films on 8-Inch Wafers . . . " Jap. Journal of Applied Physics. vol. 35, No. 9B, Part 01, Sep. 10, 1996, pp. 4875-4879.
  • Arai T., et al.: “Preparation of SrTiO3 Films on 8-Inch Wafers . . . ” Jap. Journal of Applied Physics. vol. 35, No. 9B, Part 01, Sep. 10, 1996, pp. 4875-4879.
  • Basceri, Cem et al., "The Dielectric Response as a Function of Temperature and Film Thickness of Fiber-Textured (Ba,Sr) TiO<SUB>3 </SUB>Thin Films Grown by Chemical Vapor Depostion", J. Appl. Phys. 82(5), Sep. 1, 1997, pp. 2497-2504.