US 7,006,291 B2#12785036 Most CitedExpiredUnited States (USPTO)Utility

Optical device and method for fabricating the same

8Forward Citations (#12785036 Global)
0.4/yrCitation Velocity (#19665612 Global)
2.36Citation PageRank (#11175531 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The optical device having a predetermined surface profile of the invention is fabricated by forming a multi-layered dielectric film on the surface of a solid composition layer having a glass transition temperature of not lower than 100° C. The solid composition layer is formed by molding and curing a polymerizable organic group-having fluid composition. The curing may be effected through photopolymerization or thermal polymerization of the polymerizable organic group in the composition, and a predetermined surface profile is transferred onto the composition layer from the mold used. The cured composition is released from the mold, and this is coated with a multi-layered dielectric film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An optical device comprising: a solid composition layer having a predetermined protrusion or groove surface profile on a surface thereof, wherein said solid composition layer is resin; and a multi-layered dielectric film coating the surface of the solid composition layer, wherein the solid composition layer is constituted by a layer formed by providing at least one of heat or UV light to a fluid composition containing a polymerizable organic group on a substrate so as to polymerize and cure the fluid composition.

  2. Claim 2Depends on #1

    An optical device according to claim 1 , wherein a glass transition temperature of the solid composition layer is not lower than 100° C.

  3. Claim 3Depends on #2

    The optical device as claimed in claim 2 , wherein the glass transition temperature of the solid composition is not lower than 150° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗