Static dissipative polyurethane foams
Abstract
A static dissipative flexible polyurethane foam is formed under free rise expansion conditions from a polyether graft polyol and an isocyanate, wherein one or more anti-static additives are incorporated into the reaction mix in an amount from 0.10 to 20 parts by weight. Water is added in an amount of from 0.2 to 1.0 parts per weight. Upon curing, the foam has a density in the range of 6 to 20 pounds per cubic foot, a surface resistivity below 1×10 11 ohms/square, and a pore size in the range of 100 to 250 pores per inch. The foam may be fabricated (cut or shaped) to form a shaped article, such as a roller, a clean room wipe, a cosmetic applicator or a packaging element.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for making a flexible polyurethane foam, comprising: mixing at a mix head to react (i) a polyether graft polyol or a polyether graft polyol mixed with an ester polyol and/or a polyether polyol, wherein said polyol or combination of polyols has a number average molecular weight of from about 500 to about 8000, with (ii) an isocyanate selected from the group consisting of diphenylmethane 4,4′ diisocyanate, diphenyl methane 2,2′ diisocyanate, diphenylmethmne 2,4′ diisocyanate, toluene diisocyanate, higher molecular weight isocyanate oligomers, and mixtures thereof, with an isocyanate ind
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗