Spin annealed poly(trimethylene terephthalate) yarn
Abstract
A spinning process for poly(trimethylene terephthalate) and an analytical method wherein the process provides an aging resistant poly(trimethylene terephthalate) yarn and the analytical method provides predictability to the process.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 36 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process comprising: (a) extruding melted 3GT through a spinneret; (b) quenching the extruded 3GT to form a threadline of solid filaments wherein the filaments have a tension at 130° C. greater than about 0.02 g/d; (c) passing the filaments to a heated godet operated at a speed and temperature to heat the threadline wherein the speed and temperature to which the threadline is heated are sufficient to provide a yarn with a DWS value of about 4% or less; and (d) cooling the yarn to a temperature of about 35° C. or less.
- Claim 2Depends on #1
The process of claim 1 , wherein a finish is applied to the solid filaments after quenching.
- Claim 3Depends on #1
The process of claim 1 , wherein the cooling is accomplished using a cool godet.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (36)
Non-Patent Literature (2)
- English Translation of Asashi's JP 01214372 By Z. Ding.
- International Search Report and Written Opinion (Date of Mailing: Aug. 10, 2004).