Crystalline polyester
Abstract
A crystalline polyester having a number-average molecular weight of from 5000 to 10000, a weight-average molecular weight of from 150000 to 8000000, a maximum peak temperature of heat of fusion of from 60° to 150° C., and a ratio of a softening point to a maximum peak temperature of heat of fusion (softening point/peak temperature) of from 0.6 to 1.3. The crystalline polyester can be used as a resin binder for a toner used for developing electrostatic latent images formed in electrophotography, electrostatic recording method, electrostatic printing method, and the like.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 14.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A crystalline polyester having a number-average molecular weight of from 5000 to 10000, a weight-average molecular weight of from 150000 to 8000000, a maximum peak temperature of heat of fusion of from 60° to 150° C., and a ratio of a softening point to a maximum peak temperature of heat of fusion (softening point/peak temperature) of from 0.6 to 1.3.
- Claim 2Depends on #1
The crystalline polyester according to claim 1 , wherein the crystalline polyester has a number-average molecular weight of from 5500 to 9000, a weight-average molecular weight of from 300000 to 6000000, a maximum peak temperature of heat of fusion of from 80° to 140° C., and a ratio of a softening point to a maximum peak temperature of heat of fusion (softening point/peak temperature) of from 0.9 to 1.2.
- Claim 3Depends on #1
The crystalline polyester according to claim 1 , wherein the crystalline polyester com
Technical Overview & Description