Patents
US 6,998,067 B2#123145134 Most CitedExpiredUnited States (USPTO)Utility

Method of dusting-preventive treatment of powder having dusting property

0Forward Citations (#123145134 Global)
0.0/yrCitation Velocity (#123145134 Global)
0.56Citation PageRank (#123145134 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of dusting-preventive treatment in which a powder having dusting property is treated with fibril-forming PTFE (polytetrafluoroethylene) to impart non-dusting property thereto and the non-dusting property of the powder, after having been reduced during transportation, are economically and advantageously recovered or improved through a relatively simple step. The method comprises: a first dusting-preventive treatment step in which fibril-forming polytetrafluoroethylene is added to a powder having dusting property, and a compression/shear force is exerted to the mixture at a temperature in the range of 20 to 200° C. to thereby regulate powder so as to have a flow value of 150 mm to 200 mm; and a second dusting-preventive treatment step in which a compression/shear force is exerted again at a temperature in the range of 50 to 150° C., without newly adding fibril-forming polytetrafluoroethylene, to the resultant powder after the powder treated in the first step has deteriorated in dusting-preventive property during transportation with transporting means due to such an external force that the polytetrafluoroethylene fibrils partly cleave or powder particles partly fall off polyt

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of dusting-preventive treatment of powder having dusting property comprising: a first dusting-preventive treatment step in which fibril-forming polytetrafluoroethylene is added to a powder having dusting property, and a compression/shear force is exerted to the mixture at a temperature in the range of 20 to 200° C. to thereby regulate powder so as to have a flow value of 150 mm to 200 mm; and a second dusting-preventive treatment step in which a compression/shear force is exerted again at a temperature in the range of 50 to 150° C., without newly adding fibril-forming polytetrafluoroe

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.